ASTM A516-Pressure Vessel Steel Plate

Aug 05, 2025 Leave a message

ASTM-A516-A516M-Standard-Specification.pdf

ASTM A516/ASME SA516-Pressure Vessel Steel Plate

 

Applications

 

The differences in chemical composition and mechanical properties of the different grades determine their specific use:

Gr 55:Low carbon content (≤0.27%), moderate manganese content (0.85~1.20%), good weldability and low-temperature toughness (-45℃ impact test optional). The tensile strength is 380~515 MPa and the yield strength is ≥205 MPa.

Low-temperature pressure vessels: such as liquefied natural gas (LNG) storage tanks, liquid nitrogen/liquid oxygen containers, etc., suitable for environments above -45℃.

Low-pressure vessels: atmospheric pressure storage tanks, reaction kettles, heat exchanger shells, etc.

Petrochemical equipment: desulfurization tower, distillation tower, and other scenarios with low corrosive requirements.

Boiler components: low-pressure boiler ladle, header, etc.

 

Gr 60:Slightly higher carbon content (≤0.30%), elevated manganese content (0.85~1.50%), tensile strength of 415~550 MPa, yield strength ≥220 MPa. better balance of strength and toughness.

Medium pressure vessels: separators, buffer tanks, etc. in petroleum refining.

Chemical equipment: ammonia synthesis tower, urea reactor and other occasions requiring medium strength.

Power industry: boiler ladle, superheater shell (working temperature ≤ 350 ℃).

Shipbuilding: secondary pressure-bearing parts of liquefied gas carriers.

 

Gr 65: Further increase in carbon and manganese content (C ≤ 0.31%, Mn ≤ 1.60%), tensile strength 450 ~ 585 MPa, yield strength ≥ 240 MPa. Higher strength, but the welding needs to be preheated (e.g., 150 ℃ or more).

High-pressure vessel: ammonia reactor, hydrogenation reactor and other equipment subject to high pressure.

Energy equipment: high-temperature and high-pressure parts of power station boilers (need to be used with heat insulation layer).

Heavy-duty storage tanks: reinforcement rings or top plates of large petroleum storage tanks.

Low-temperature applications: -60℃ impact requirements can be met through normalizing treatment, used for polar equipment.

 

Gr 70:Highest strength grade (tensile strength 485~620 MPa, yield strength ≥260 MPa), but plasticity and weldability are relatively reduced, requiring strict control of the welding process.

Extreme pressure environments: high pressure gas storage tanks (e.g. CNG tanks), auxiliary pressure vessels for nuclear power plants.

Heavy-duty structures: support frames or high-strength shells for large chemical equipment.

Special applications: mobile pressure vessels (e.g. tank trucks) where weight reduction is required, thinning of wall thickness through high strength.

 

Chemical Requirements

 

Elements SA 516 Gr 55
(Grade 380)
SA 516 Gr 60
(Grade 415)
SA 516 Gr 65
(Grade 450)
SA 516 Gr 70
(Grade 485)
Carbon, max Composition %        
1/2 in. (12.5 mm) and under 0.18 0.21 0.24 0.27
Over 1/2 to 2 in. (12.5 to 50 mm), incl 0.20 0.23 0.26 0.28
Over 2 to 4 in. (50 to 100 mm), incl 0.22 0.25 0.28 0.30
Over 4 to 8 in. (100 to 200 mm), incl 0.24 0.27 0.29 0.31
Over 8 in. (200 mm) 0.26 0.27 0.29 0.31
Manganese, max        
1/2 (12.5) and under:        
Heat analysis 0.60-0.90 0.60-0.90 0.85-1.20 0.85-1.20
Product analysis 0.55-0.98 0.55-0.98 0.79-1.30 0.79-1.30
Over 1/2 in (12.5)        
Heat analysis 0.60-1.20 0.85-1.20 0.85-1.20 0.85-1.20
Product analysis 0.55-1.30 0.79-1.30 0.79-1.30 0.79-1.30
Phosphorus, max 0.025 0.025 0.025 0.025
Sulfur, max 0.025 0.025 0.025 0.025
Silicon        
Heat analysis 0.15-0.40 0.15-0.40 0.15-0.40 0.15-0.40
Product analysis 0.13-0.45 0.13-0.45 0.13-0.45 0.13-0.45

 

 

 

Mechanical Properties

 

Grade Tensile strength, ksi(MPa) Yield strength, min.B ksi (MPa) Elongation in 8 in. (200 mm), min, % Elongation in 2 in. (50 mm), min, %
SA516 Gr. 55 55-75[380-515] 30[205] 23 27
SA516 Gr. 60 60-80[415-550] 32[220] 21 25
SA516 Gr. 65 65-85[450-585] 35[240] 19 23
SA516 Gr. 70 70-90[485-620] 38[260] 17 21

 

Heat Treatment and Tempering

 

The factors that affect the heat treatment method generally include: thickness, impact toughness requirements, and welding process. The specific levels are as follows

news-1-1

1. SA516 Gr.55:

As-Rolled: Applicable to thinner steel plates (usually ≤40mm), used directly after rolling without additional heat treatment.

Normalizing: Normalizing can be performed if it is necessary to improve the uniformity of the structure or meet special impact requirements.

Normalizing + tempering (N+T): Used for thick plates (such as ≥50mm) or when low-temperature toughness is required.

2. SA516 Gr.60

Hot rolling (As-Rolled): Applicable to steel plates with a thickness of ≤40mm.

Normalizing: Applicable to thickness of 40mm~100mm, or when impact toughness needs to be improved.

Normalizing + tempering (N+T): Applicable to plates with a thickness of ≥100mm or low temperature (such as -46°C) impact requirements.

 

news-1-1

3. SA516 Gr.65

Hot rolling (As-Rolled): only applicable to thin plates ≤20mm (must meet mechanical properties).

Normalizing: applicable to 20mm~75mm thickness, to ensure uniformity of structure.

Normalizing + tempering (N+T): applicable to thick plates ≥75mm or low temperature impact requirements (such as -46°C).

4. SA516 Gr.70

Normalizing (Normalizing is required for almost all thicknesses): Applicable to steel plates ≤75mm

Normalizing + Tempering (N+T): Applicable to thick plates ≥75mm or with strict low-temperature toughness requirements.

 

 

ABOUT US

 

GNEE has extremely strict requirements for product quality and production safety. All products have passed international safety certifications and comply with relevant industry safety standards. We always put customer safety first, ensuring that every piece of equipment is highly safe and reliable.

If you want to know about certain products, you can send an email to alloy@gneesteelgroup.com.