What SA516 Gr 70 Is and Which Standards Apply
SA516 Gr 70 is a carbon steel plate for pressure vessels covered by ASTM A516/A516M and, with identical technical content, by ASME SA-516 in Section II Part A. The designation combines the tensile class - 70 ksi, equivalent to 485 MPa - with the product family that also contains Grades 55, 60 and 65. Plates are melted in the oxygen converter or electric furnace, are fully killed and fine grained, and are supplied as-rolled, normalized, or normalized and stress relieved. ASTM A516/A516M requires normalization for Grades 60, 65 and 70 once thickness passes 40 mm, because the coarse as-rolled structure of heavy plate reduces notch toughness.
Chemical Composition and Mechanical Properties
The grade is a plain C-Mn steel, so the property balance depends on tight control of carbon, manganese and residuals rather than on alloying additions.
| Element | Heat analysis requirement |
|---|---|
| C | 0.28 % max up to 12.7 mm; 0.30 % max over 12.7 to 50 mm |
| Mn | 0.85-1.20 % up to 12.7 mm; 0.79-1.30 % over 12.7 mm |
| Si | 0.15-0.40 % (0.13-0.45 % for fully killed plate) |
| P | 0.035 % max |
| S | 0.035 % max |
| Yield strength (min) | 260 MPa |
| Tensile strength | 485-620 MPa |
| Elongation (50 mm gauge) | 21 % min for plate up to 20 mm |
Impact testing is supplementary: when it is ordered, the Charpy V-notch test temperature is agreed at enquiry, and -46 °C is the value most frequently requested for low-temperature service. Plates supplied with impact qualification carry the corresponding test temperature and absorbed energy on the mill certificate.
Service Envelope and Typical Applications
SA516 Gr 70 is designed for moderate and lower temperature pressure service, and it remains the default shell, head and nozzle-reinforcement material for a very wide range of static equipment. Typical applications include hydrotreater and hydrocracker shells, LPG storage spheres, boiler drums and steam headers, heat exchanger shells and channels, separators and knockout drums, ammonia and methanol plant vessels, air receiver tanks and water turbine volute casings. The grade is favoured because its strength, ductility and weldability are balanced at a modest cost, and because it is recognized by both ASME and EN-oriented construction codes.
Delivery Condition, Testing and Supply Scope
Plate is produced from 5 mm to 200 mm in cut-to-length or coil-derived formats. As-rolled supply is normal up to 40 mm; above that thickness normalized or normalized plus stress relieved plate is the standard offer. Mill certification is issued to EN 10204 type 3.1, with type 3.2 available when third-party witnessing is required, and every plate is marked with its heat number, grade and plate identification traceable to the certificate. Ultrasonic examination is performed to ASTM A578 Level 1 or 2, or to EN 10160 class S1/E1 for thicker plate, and dimensional and surface inspection reports are provided with each consignment. Cutting to size, edge beveling and rolling into shell courses can be carried out before shipment.
Fabrication and Welding Notes
SA516 Gr 70 welds with conventional carbon steel processes. Low-hydrogen consumables of the AWS A5.1 E7018 or AWS A5.20 E71T-1 classification are appropriate for shielded metal arc and flux-cored welding, and submerged arc welding with neutral fluxes is standard for long seams. Preheat of roughly 100-150 °C is applied once thickness exceeds about 25 mm, and interpass temperature is normally held below 250 °C. Post-weld heat treatment, when required by the construction code, is carried out in the 595-650 °C range, holding time based on thickness and cooling controlled to limit residual stress. Cold forming is straightforward, but formed strain above roughly 5 % should be followed by stress relief when the design code demands it. Three points are often confused at enquiry stage: A515 grades are intended for intermediate and higher temperature service and carry no low-temperature impact guarantee, whereas A516 plate is killed and fine grained; the tensile class number is not a yield value; and normalization is required above 40 mm rather than being an optional upgrade.
Frequently Asked Questions
Q: What is the difference between SA516 Gr 70 and SA515 Gr 70?
A: A515 covers carbon steel plate for intermediate and higher temperature service, while A516 covers moderate and lower temperature service. A516 plate is fully killed and fine grained and is routinely ordered with Charpy impact tests; A515 grades are not produced with a low-temperature impact guarantee.
Q: What tensile strength does SA516 Gr 70 have?
A: The specified tensile range is 485-620 MPa, with a minimum yield strength of 260 MPa measured as 0.2 % offset for the normalized condition.
Q: Which thicknesses must be normalized?
A: ASTM A516/A516M requires normalization for Grades 60, 65 and 70 when the plate thickness exceeds 40 mm. Below that thickness as-rolled plate is normally acceptable if it meets the compositional and mechanical limits.
Q: Can SA516 Gr 70 be used at -46 °C?
A: It can be supplied with impact testing at -46 °C and accepted at that temperature when the applicable construction code allows it. For permanent service at very low temperature, low-alloy grades with a documented low-temperature design curve are usually the more economical and safer choice.
Q: What documents accompany a shipment?
A: An EN 10204 type 3.1 mill certificate listing heat analysis, tensile and impact results, plate identification marking traceable to the certificate, ultrasonic examination reports where ordered, and dimensional inspection records.
Q: Is SA516M Gr 70 different from SA516 Gr 70?
A: The M suffix identifies the metric edition of the specification. Grade requirements are the same; only the expression of dimensions and units differs.