The higher steel grade ABS Grade FH40,ABS FH40 ship plate,ABS FH40 steel plate are used abnormally owning to its high cost and substitutability.With the minimum yield point at 390 Mpa,and tensile strength within 510-650 Mpa,steel plate ABS Grade FH40 can bear the higher strength and used to some steel structure parts in ships.
Steel Standard:ABS (American Bureau of Shipping)
Rolling Type:Shipbuilding steel plate,High tension ship plate
Thickness:6mm-250mm
Width:1500mm-4200mm
Length:3000mm-18000mm
Heat Treatment:TMCP/Normalized
Technical Requirements & Additional Services for ABS FH40 steel plate:
High tension test
Z-Test (Z15,Z25,Z35)
Low temperature impacting test
Ultrasonic test under ASTM A435,A577,A578
Cetificated by ABS,LR,GL,BV,DNV,KR,NK,CCS,RINA
Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
Shot blasting and Painting,Cutting and welding as per end user's demands
|
ABS FH40 high Strength Chemical Composition |
|||||||
|
Grade |
The Element Max (%) |
||||||
|
C |
Si |
Mn |
P |
S |
Al |
N |
|
|
ABS FH40 |
0.16 |
0.1-0.50 |
0.90-1.6 |
0.025 |
0.025 |
0.015 |
0.009 |
|
Nb |
V |
Ti |
Cu |
Cr |
Ni |
Mo |
|
|
0.02-0.05 |
0.05-0.10 |
0.02 |
0.35 |
0.2 |
0.8 |
0.08 |
|
Crack Sensitivity: Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent: Ceq = 【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%
|
ABS FH40 high strength property |
|||||||
|
Grade |
|
Mechanical Property |
Charpy V Impact Test |
||||
|
Thickness |
Yield |
Tensile |
Elongation |
Degree |
Energy 1 |
Energy 2 |
|
|
ABS FH40 |
mm |
Min Mpa |
Mpa |
Min % |
-60 |
J |
J |
|
t≤50 |
390 |
510-650 |
20% |
26 |
39 |
||
|
50<t≤70 |
390 |
510-650 |
20% |
31 |
46 |
||
|
70<t≤100 |
390 |
510-650 |
20% |
37 |
55 |
||
|
Note: Energy 1 is transverse impact test, Energy 2 is longitudinal |
|||||||