14Cr1MoR Pressure Vessel Steel Plate for Service to 500 C

Mar 01, 2024 Leave a message

Grade Identity and Field of Use

14Cr1MoR is a chromium molybdenum steel plate defined by GB/T 713-2014, the Chinese standard for pressure vessel plates. The designation records the nominal carbon content of 0.14 percent, the chromium and molybdenum additions, and the letter R for the vessel plate family. The grade belongs to the group of heat resistant, hydrogen resistant steels used for medium temperature pressure equipment, and its service range extends to about 500 degrees Celsius.

The reason for using a chromium molybdenum steel rather than a plain carbon vessel steel is the behaviour of the material at temperature and in a hydrogen bearing process stream. At elevated temperature and pressure, hydrogen can diffuse into carbon steel, react with carbides and cause internal decarburisation and fissuring. Chromium and molybdenum stabilise the carbides and make the steel resistant to that attack, so the two elements are what allow this grade to be used in hydroprocessing, reforming and similar services.

Chemical Composition and Steelmaking

The analysis is tightly banded and the steel is produced through a clean steelmaking route: electric furnace melting followed by ladle refining and vacuum degassing. Vacuum treatment lowers hydrogen and nitrogen, and careful control of residual elements such as tin, antimony, arsenic and copper reduces the tendency to temper embrittlement, which is the loss of toughness that can occur in chromium molybdenum steels during long exposure at elevated temperature.

Element Typical heat analysis (percent) Function
Carbon 0.11 to 0.17 Strength and carbide formation
Silicon 0.15 to 0.40 Deoxidation
Manganese 0.40 to 0.70 Hardenability and strength
Chromium 1.15 to 1.50 Resistance to hydrogen attack and oxidation
Molybdenum 0.45 to 0.65 Creep strength and carbide stability
Phosphorus and sulphur held at low residual levels Purity and resistance to temper embrittlement

Delivery Condition and Mechanical Requirements

14Cr1MoR is supplied in a heat treated condition, normally quenched and tempered or normalised and tempered according to the thickness and the intended forming route. The mechanical requirement covers tensile strength in the 515 to 690 MPa range, a minimum yield strength of 310 MPa at room temperature, a minimum elongation of 18 percent and Charpy V-notch impact energy of not less than 34 J at 20 degrees Celsius. Hardness in the delivered condition is typically in the range of 150 to 200 HBW, which keeps the plate machinable while reflecting the tempered structure.

Because the plate is used for pressure retaining components, the certificate reports additional information: elevated temperature yield strength values used for design at the working temperature, the heat treatment cycle, and where specified the results of impact testing taken from the quarter thickness position. Plates can be ordered with through thickness Z15, Z25 or Z35 quality for nozzle and support connections that develop high through thickness stress.

Production Route and Heat Treatment

The typical manufacturing sequence is electric furnace melting, ladle furnace refining, vacuum degassing, ingot or slab casting, rolling to plate, ultrasonic examination, normalising, tempering, finishing and final inspection. Each step contributes to the result: vacuum degassing controls hydrogen, controlled rolling and normalising refine the grain, and tempering develops the required balance of strength and toughness.

Smelting: electric furnace with ladle refining and vacuum degassing.

Rolling: controlled schedules to achieve the required properties in heavy plate.

Heat treatment: quenched and tempered or normalised and tempered.

Examination: ultrasonic testing to confirm internal soundness, with acceptance levels agreed for the project.

Applications in Process and Power Plants

The grade is used in petroleum refining, petrochemical production, fertiliser plants and power generation. Typical components include the shells and heads of hydrotreating and hydrocracking reactors, heat exchanger shells, separator and drum shells, high pressure steam piping components, turbine cylinder casings, coal gasification equipment and pressure retaining parts of equipment handling hydrogen or hydrogen mixed process gas.

Components are fabricated by welding heavy sections, and after welding the assemblies are given a post weld heat treatment at a temperature appropriate to the steel so that residual stress is reduced without damaging the properties developed by the original heat treatment. Because the steel is used in hydrogen service, the fabrication sequence also includes hardness control on weldments, since excessive hardness in the heat affected zone is a known risk factor in this class of equipment.

Quality Control and Fabrication Notes

Cutting is carried out by flame, plasma or waterjet, with preheat applied to thicker sections. Cold forming is preferred where geometry allows; hot forming requires a subsequent normalising and tempering treatment because the working temperature destroys the original structure. Welding uses matching chromium molybdenum consumables, low hydrogen practice, preheat in the 150 to 200 degrees Celsius range and interpass temperature control, with post weld heat treatment applied according to the qualified procedure.

Quality control covers chemical analysis per heat, tensile and impact testing, ultrasonic examination of the plate and of welded joints, hardness surveys of weldments, dimensional inspection and full heat number traceability. Documentation is normally prepared for a notified inspection body, and the plate carries marking that allows each piece to be traced back to its heat and its heat treatment batch throughout the life of the vessel.

Frequently Asked Questions

Q: What is the maximum service temperature of 14Cr1MoR?

A: The grade is applied in medium temperature service up to about 500 degrees Celsius, with design values taken from elevated temperature data in the applicable standard.

Q: Why is chromium added to this steel?

A: Chromium stabilises carbides and gives resistance to hydrogen attack and oxidation at elevated temperature, which is the key requirement in hydroprocessing service.

Q: In what condition is the plate delivered?

A: Quenched and tempered or normalised and tempered, with the cycle recorded on the mill test certificate.

Q: Which through thickness qualities can be supplied?

A: Z15, Z25 and Z35 are available, and they are ordered together with ultrasonic testing for restrained welded connections.

Q: Why are residual elements controlled so closely?

A: Because tin, antimony, arsenic and copper promote temper embrittlement during long service at elevated temperature, which reduces toughness.

Q: Is post weld heat treatment required?

A: It is normally required for heavy welded pressure components, and the temperature is selected to relieve stress while preserving the properties of the plate.