Product Item: Alloy Steel Plate
Material: ASTM A387 Grade 91 Class 2
Sizes: 1800 x 8000 x 8 mm
The Alloy Steel Plate is crafted from ASTM A387 Grade 91 Class 2, offering excellent strength and resistance to high temperatures.
With a width of 1800 mm, length of 8000 mm, and thickness of 8 mm, this plate is ideal for use in industries requiring durable materials for high-pressure and high-temperature applications.
Our ASTM A387 Supply Range:
Description: Chrome Moly Alloy Steel Plate ASME SA387/ ASTM A387
Grade: A/SA387 GRADE 11, 22, 12, 5, 9, 91
Manufacturing Types: Hot Rolled, Heat Treated
Thickness: 5 to 150 mm
Width: 0.6m to 3m
Length: 6m, 12m, customized
Surface: Natural, Painted
Packing: Standard sea packing, bundled with streel strip.
Customized cutting: Laser Cut, Plasma Cut, CNC Cut.
ASTM A387 GR 91 CLASS 2 Chemical Composition
| Grade | C | Mn | P | S | Si | Cr | Mo | V |
|---|---|---|---|---|---|---|---|---|
| A387 Gr.91 | 0.08-0.12 | 0.30-0.60 | 0.020 | 0.010 | 0.20-0.50 | 8.00-9.50 | 0.85-1.05 | 0.18-0.25 |
ASTM A387 / SA387 GR 91 CLASS 2 Mechanical Properties
| Class | Tensile (MPa) | Yield (MPa) | Elong. (50mm) | Elong. (200mm) | Reduc'n of Area* |
|---|---|---|---|---|---|
| Class 2 | 585 - 760 | 415 min | 18% min | - | - |
Equivalent Grades for ASME SA387 Grade 91 Alloy Steel Plates Class 2 Plates
| COUNTRY | USA | EUROPEAN | GERMANY | ENGLAND | FRANCE | RUSSIA |
|---|---|---|---|---|---|---|
| STANDARDS | ASTM | EN 10028 | DIN | BS | AFNOR 36206 | GOST |
| Grade 91 | A387 | 10CrMoVNb9-1 | - | - | - | - |
Overview SA 387 Gr 12 / SA 387 Gr 5 / SA 387 Gr 9 / SA 387 Gr 91
Certain applications with the Refining and Power Industries along with specific environments within Chemical Plants require grades which address limited corrosion and elevated temperature concerns.
SA 387 Gr 12 is utilized to address low to moderate temperature challenges. For conditions with higher elevated operating temperatures, our SA 387 Gr 5, SA 387 Gr 9 and SA 387 Gr 91 are often used. Minimum tempering temperature for these cr / mo grades are:
SA 387 Gr 12 (1150 °F)
SA 387 Gr 9 (1250 °F)
SA 387 Gr 5 (1300 °F)
SA 387 Gr 91 (1350 °F)
Thickness' from 3/16″ – 6″
Supplemental testing available to simulate application and environment conditions
These grades can be specified in either Class 1 or Class 2
Computer controlled processing per customer specifications
In the tables use SA 387 Gr 12, SA 387 Gr 5, SA 387 Gr 9, and SA 387 Gr 91
Chemical Requirements
*Elements represented in percentage
| Element Composition % | ||||
|---|---|---|---|---|
| SA 387 Grade 12 |
SA 387 Grade 5 |
SA 387 Grade 9 |
SA 387 Grade 91 |
|
| Carbon, max: | ||||
| Heat analysis | 0.05-0.17 | 0.15 max | 0.15 max | 0.08-0.12 |
| Product analysis | 0.04-0.17 | 0.15 max | 0.15 max | 0.06-0.15 |
| Manganese, max: | ||||
| Heat analysis | 0.40-0.65 | 0.30-0.60 | 0.30-0.60 | 0.30-0.60 |
| Product analysis | 0.35-0.73 | 0.25-0.66 | 0.25-0.66 | 0.25-0.66 |
| Phosphorus, max: | ||||
| Heat analysis | 0.025 | 0.025 | 0.025 | 0.020 |
| Product analysis | 0.025 | 0.025 | 0.025 | 0.025 |
| Sulfur, max: | ||||
| Heat analysis | 0.025 | 0.025 | 0.025 | 0.010 |
| Product analysis | 0.025 | 0.025 | 0.025 | 0.012 |
| Silicon: | ||||
| Heat analysis | 0.15-0.40 | 0.50 max | 1.00 max | 0.20-0.50 |
| Product analysis | 0.13-0.45 | 0.55 max | 1.05 max | 0.18-0.56 |
| Chromium: | ||||
| Heat analysis | 0.80-1.15 | 4.00-6.00 | 8.00-10.00 | 8.00-9.50 |
| Product analysis | 0.74-1.21 | 3.90-6.10 | 7.90-10.10 | 7.90-9.60 |
| Molybdenum: | ||||
| Heat analysis | 0.45-0.60 | 0.45-0.65 | 0.90-1.10 | 0.85-1.05 |
| Product analysis | 0.40-0.65 | 0.40-0.70 | 0.85-1.15 | 0.80-1.10 |
Tensile Requirements For Class 1 Plates
| SA 387 Grade 12 |
SA 387 Grade 22, 5, 9 |
|
|---|---|---|
| Tensile strength, ksi [MPa] | 55 to 80 [380 to 550] |
60 to 85 [415 to 585] |
| Yield strength min. ksi [MPa] | 33 | 30 |
| Elongation in 8 in. [200 mm], min. % | 18 | |
| Elongation in 2 in. [50 mm], min. % | 22 | 18 |
| Reduction of area, min % | 45 40 |
Tensile Requirements For Class 2 Plates
| SA 387 Grade 12 |
SA 387 Grade 5, 9 |
SA 387 Grade 91 |
|
|---|---|---|---|
| Tensile strength, ksi [MPa] | 65 to 85 [450 to 585] |
75 to 100 [515 to 690] |
85 to 110 [585 to 760] |
| Yield strength min. ksi [MPal]/(0.2% offset) | 40 [275] | 45 [310] | 60 [415] |
| Elongation in 8 in. [200 mm], min. %B | 19 | … | … |
| Elongation in 2 in. [50 mm], min. %B | 22 | 18 | 18 |
| Reduction of area, min % | … | 45 40 |
… |