The difference between RINA D420 and RINA D460 steel plate

Apr 10, 2026 Leave a message

RINA D420 is an extra-high-strength marine steel plate certified by the Italian classification society RINA (Registro Italiano Navale) for shipbuilding and offshore applications. The "D" grade signifies it is impact tested at -20°C . It has a minimum yield strength of 420 MPa and tensile strength ranging from 530 to 680 MPa, with a minimum elongation of 18% . The chemical composition is strictly controlled with carbon ≤0.20%, manganese ≤1.70%, and microalloying elements . This grade is typically supplied in normalized, quenched and tempered (QT), or TMCP conditions and is available in thicknesses up to 260mm . It is widely used for hull structures, offshore platforms, and critical marine engineering components .

 

RINA D460 is an extra-high-strength marine steel plate also certified by RINA, with impact toughness tested at -20°C . The "460" denotes a minimum yield strength of 460 MPa and tensile strength ranging from 570 to 720 MPa, with a minimum elongation of 17% . Impact energy requirements are minimum 31J (transverse) and 46J (longitudinal) at -20°C . The chemical composition features carbon ≤0.21%, manganese ≤1.70%, with strict control of phosphorus and sulfur . This grade is designed for demanding structural components in shipbuilding, offshore platforms, and Arctic-class vessels requiring superior strength-to-weight ratio .

 

Both RINA D420 and RINA D460 are RINA-certified extra-high-strength marine steels with excellent low-temperature toughness tested at -20°C, ensuring reliable performance in harsh marine environments . Their primary difference lies in strength level: D420 offers a minimum yield strength of 420 MPa with tensile strength of 530-680 MPa, suitable for high-strength offshore platforms and general shipbuilding , while D460 provides a higher minimum yield strength of 460 MPa with tensile strength reaching 570-720 MPa, designed for more demanding load-bearing applications requiring superior strength-to-weight ratio . Both grades feature controlled chemical composition with carbon ≤0.20-0.21% and maintain good weldability for critical marine service, with D460 typically requiring more precise processing to achieve its enhanced mechanical properties . The selection between them depends on whether the project requires the balanced strength of D420 or the enhanced performance of D460 for more extreme structural demands .

 

RINA D420 extra high Strength Chemical Composition in Tempering and Quenching

 

Element

RINA D420 Max %

Element

RINA D420 Max %

C

0.20

Ni

0.40

Mn

1.70

Mo

0.08

Si

0.10-0.55

Al

0.020 min

S

0.030

Nb

0.20-0.05

P

0.030

V

0.05-0.10

Cu

0.35

Ti

0.0007-0.05

Cr

0.20

N

 

 

RINA D460 extra high Strength Chemical Composition in Tempering and Quenching

 

Element

RINA D460 Max %

Element

RINA D460 Max %

C

0.20

Ni

0.40

Mn

1.70

Mo

0.08

Si

0.10-0.55

Al

0.020 min

S

0.030

Nb

0.20-0.05

P

0.030

V

0.05-0.10

Cu

0.35

Ti

0.0007-0.05

Cr

0.20

N

 

 

RINA D420 extra high strength property in Tempering and Quenching

 

Grade

Thickness

Yield Strength

Tensile Strength

Elongation

Impact Energy

(mm)

MPa (min)

MPa

% (min)

(KV J) (min)

 

 

 

 

-20 degree

RINA D420

8-260

420

530-680

18

28J

 

RINA D460 extra high strength property in Tempering and Quenching

 

Grade

Thickness

Yield Strength

Tensile Strength

Elongation

Impact Energy

(mm)

MPa (min)

MPa

% (min)

(KV J) (min)

 

 

 

 

-20 degree

RINA D460

8-260

460

570-720

17

31J