SA517 Grade P is a specific grade of high-strength, quenched and tempered alloy steel plate conforming to the ASME SA-517 standard, designed for fusion-welded boilers and pressure vessels, and noted for its elevated physical properties and suitability for use in low-temperature applications. It features a particular chemical composition that includes carbon, silicon, manganese, nickel, chromium, molybdenum, and boron, among other elements, which contribute to its strength and ductility.
SA517 grade P Chemical Composition
|
SA517 grade P Chemical Composition |
||||||
|
Grade |
The Element Max (%) |
|||||
|
C |
Si |
Mn |
P |
S |
Ni |
|
|
SA517 grade P |
0.10-0.23 |
0.18-0.37 |
0.40-0.78 |
0.035 |
0.035 |
1.15-1.55 |
|
Cr |
Mo |
B |
|
|
|
|
|
0.79-1.26 |
0.41-0.64 |
0.001-0.005 |
|
|
|
|
Carbon Equivalent: Ceq = 【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%
SA517 grade P Mechanical Property
|
Grade |
|
SA517 grade P Mechanical Property |
||
|
Thickness |
Yield |
Tensile |
Elongation |
|
|
SA517 grade P |
mm |
Min Mpa |
Mpa |
Min % |
|
6-65 |
690 |
795-930 |
16% |
|
|
65-150 |
620 |
725-930 |
14% |
|
Key Characteristics and Applications
High-Strength Quenched and Tempered Alloy Steel:
This classification indicates that the steel has undergone a heat treatment process (quenching and tempering) to significantly increase its strength and toughness.
Pressure Vessel Applications:
SA517 Grade P is primarily used in the construction of fusion-welded boilers and other high-pressure equipment where high strength and good ductility are essential.
Low-Temperature Service:
The alloy's composition makes it suitable for subzero and cryogenic applications, with the potential to operate at temperatures as low as -75°F [-59°C].