ASTM A709 Grade 36 Steel Plate: Properties, Chemistry and Plate Sizes

Sep 08, 2025 Leave a message

ASTM-A709-A709M-21.pdf

ASTM A709 Grade 36 Steel Plate for Bridge Construction

ASTM A709 is the standard specification for structural steel for bridges. It gathers carbon steel, high strength low alloy steel and quenched and tempered alloy steel plate into a single document so that bridge designers can select a material by strength, toughness and corrosion resistance from one family of grades. Grade 36 is the carbon steel base grade of that family and is the material most widely used for welded bridge girders, cross frames, bearing stiffeners and secondary members.

In the metric portion of the specification the same material appears as Grade 250, named after its minimum yield strength in megapascals. Grade 36 takes its name from the equivalent requirement in kilopounds per square inch, so the two designations describe one steel with a minimum yield strength of 36 ksi or 250 MPa.

Chemical Composition Requirements

Composition limits for Grade 36 depend on the plate thickness being rolled. Thin plate is held to a simple carbon-manganese specification with no minimum manganese requirement, while thicker plate has a manganese range added so that strength is maintained through the section. Copper is specified as a minimum when copper bearing steel is ordered for improved atmospheric corrosion resistance.

Thickness range (in) Thickness range (mm) C max (%) Mn (%) P max (%) S max (%) Si (%) Cu min (%)
0.1875-0.750 4.8-19.0 0.25 No requirement 0.030 0.030 0.40 max 0.20
0.751-1.500 19.1-38.0 0.25 0.80-1.20 0.030 0.030 0.40 max 0.20
1.501-2.500 38.1-63.5 0.26 0.80-1.20 0.030 0.030 0.15-0.40 0.20
2.501-3.000 63.5-76.2 0.27 0.80-1.20 0.030 0.030 0.15-0.40 0.20

The carbon maximum rises slightly with thickness because heavier sections need more carbon and manganese to reach the required strength after rolling. For each reduction of 0.01% in carbon below the specified maximum, an increase of 0.06% manganese above the specified maximum is permitted, up to a maximum of 1.35% manganese. The copper minimum applies when copper steel is specified on the order.

Available Plate Dimensions

Plates are produced in the sizes summarised below. The dimensions of the metric portion of the specification are the same sizes expressed in millimetres.

Grade Thickness (in) Width (in) Length (in)
36 0.1875-3.00 72-120 240-1200
36T 0.1875-3.00 72-120 240-1200
36F 0.1875-2.00 72-120 240-1200

In metric terms the plate thickness range is about 4.8 mm to 76.2 mm for Grades 36 and 36T and 4.8 mm to 50.8 mm for Grade 36F, with widths from about 1830 mm to 3050 mm and lengths from about 6100 mm to 30500 mm.

Mechanical Properties

Tensile testing is performed in the transverse direction in accordance with ASTM A370. All three variants of the grade share the same strength requirement, which is summarised below.

Grade Yield strength, min (ksi) Yield strength, min (MPa) Tensile strength (ksi) Tensile strength (MPa) Elongation in 2 in, min (%) Elongation in 8 in, min (%)
36 36 250 58-80 400-550 23 20
36T 36 250 58-80 400-550 23 20
36F 36 250 58-80 400-550 23 20

Yield strength is measured as the 0.2% offset or as 0.5% extension under load. For plates wider than 24 in, the elongation requirement is reduced by two percentage points, which is the adjustment given in the tension test section of ASTM A6, the general requirements specification that governs the tolerances of this product.

Toughness Options and Tolerances

Grade 36 is published in three forms that differ in toughness testing. Plain Grade 36 carries no Charpy V-notch requirement. Grade 36T is the toughness tested grade for non fracture critical members, and Grade 36F is the grade used for fracture critical members, where a higher minimum Charpy V-notch energy is demanded. Charpy testing for the T and F grades is carried out in the three service temperature zones defined in the specification, and the zones are reported on the mill certificate along with the test temperature actually used.

Thickness, width and length tolerances are taken from the general requirements of ASTM A6. The flatness tolerance for plate supplied in the as-supplied condition is one half of the standard ASTM A6 tolerance, which reflects the tighter geometry expected in bridge fabrication shops, where plate is cut and fitted into welded girders with little allowance for reworking.

FAQ

Q: What is ASTM A709 Grade 36 steel plate?
It is the carbon steel base grade of the bridge structural steel specification ASTM A709/A709M. In the metric system the same material is designated Grade 250, and it is specified primarily for welded bridge structures.

Q: What does the F or T suffix mean?
The suffix identifies the toughness option. Grade 36T is Charpy V-notch tested for non fracture critical members, while Grade 36F is intended for fracture critical members and must meet a higher minimum impact energy.

Q: When is copper steel ordered?
Copper is specified as a minimum of 0.20% when the designer wants the improved atmospheric corrosion resistance of copper bearing steel. The requirement is noted on the order because it changes the composition specified.

Q: How does thickness affect the requirements?
Thicker plate has a higher carbon maximum and a specified manganese range, because heavier sections need more alloy to reach the same strength. Elongation for plates wider than 24 in is reduced by two percentage points as permitted by ASTM A6.

Q: Which sizes can be supplied?
Grades 36 and 36T are rolled from 0.1875 in to 3.00 in thick and Grade 36F from 0.1875 in to 2.00 in, in widths of 72 in to 120 in and lengths of 240 in to 1200 in, with the same sizes available in metric units.

Q: Are test certificates supplied?
Yes. Each plate is delivered with a mill test certificate that records the heat number, chemical analysis, heat treatment and the tensile and impact results of the plates supplied, together with the applicable temperature zone for toughness tested grades.