ASTM A387 steel plate is a specification for chromium-molybdenum alloy steel plates intended primarily for use in elevated temperature service. These plates are designed for applications that require improved mechanical properties and resistance to oxidation, making them suitable for use in high-temperature environments.
Key Properties
Composition: ASTM A387 steel plates typically contain chromium (up to 9% or more) and molybdenum (up to 2.25% or more), which enhance their strength and corrosion resistance at high temperatures.
Grades: The specification includes various grades, such as Grade 5, 9, 11, 12, 22, and 24, differentiated by their composition and intended use.
Applications
ASTM A387 steel plates are commonly used in:
- Pressure vessels
- Heat exchangers
- Power generation equipment
- Piping systems in the oil and gas industry
- Chemical processing facilities
Overall, ASTM A387 steel plates are essential for applications requiring materials that can withstand high temperatures and corrosive environments, offering reliable performance and durability.
Chrome moly plates under ASTM A387 are available in several grades with varying alloy compositions. The commonly used grades include Gr 11, Gr 22, Gr 5, Gr 9, and Gr 91.
|
Grade |
Nominal Chromium Content, % |
Nominal Molybdenum Content, % |
|---|---|---|
|
2 |
0.50 |
0.50 |
|
12 |
1.00 |
0.50 |
|
11 |
1.25 |
0.50 |
|
22, 22L |
2.25 |
1.00 |
|
21, 21L |
3.00 |
1.00 |
|
5 |
5.00 |
0.50 |
|
9 |
9.00 |
1.00 |
|
91 |
9.00 |
1.00 |
With the exception of Grades 21L, 22L, and 91, each grade is offered in two classes based on tensile strength levels as outlined in the tensile requirements tables. Grades 21L and 22L are available only in Class 1, while Grade 91 is available solely in Class 2.
Heat Treatment for A387 Chrom Moly Alloy Steel Plate
Chrome moly alloy steel plates under ASTM A387 must be killed steel and are thermally treated through processes such as annealing, normalizing, and tempering. Alternatively, if agreed upon by the buyer, the plates may undergo accelerated cooling from the austenitizing temperature via air blasting or liquid quenching, followed by tempering.
The minimum tempering temperatures are outlined in the table below:
|
Grade |
Temperature, °F [°C] |
|---|---|
|
2, 12 and 11 |
1150 [620] |
|
22, 22L, 21, 21L and 9 |
1250 [675] |
|
5 |
1300 [705] |
Grade 91 alloy steel plates shall be heat treated by normalizing and tempering or by accelerated cooling by air blasting or liquid quenching, followed by tempering. Grade 91 plates need to be austenitized at 1900 to 1975°F [1040 to 1080°C] and shall be tempered at 1350 to 1470°F [730 to 800°C]
Grade 5, 9, 21, 21L, 22, 22L, and 91 plates ordered without heat treatment by above table, shall be finished in either the stress relieved or annealed condition.
A387 Chrom Moly Plate Data Sheet
Chemical Composition
- Table 1: For A387 Gr 11, 22, 5, 9, 91 Chrome Alloy Steel Plate
| Element | Analysis Type | Grade 12 K11757 | Grade 11 K11789 | Grade 22 K21590 | Grade 22L K21590 |
|---|---|---|---|---|---|
| Carbon: | Heat analysis | 0.05-0.17 | 0.05-0.17 | 0.05<sup>A</sup> | 0.10 max |
| Product analysis | 0.04-0.17 | 0.04-0.17 | 0.04<sup>A</sup> | 0.12 max | |
| Manganese: | Heat analysis | 0.40-0.65 | 0.40-0.65 | 0.30-0.60 | 0.30-0.60 |
| Product analysis | 0.35-0.73 | 0.35-0.73 | 0.25-0.66 | 0.25-0.66 | |
| Phosphorus, max: | Heat analysis | 0.025 | 0.025 | 0.025 | 0.025 |
| Product analysis | 0.025 | 0.025 | 0.025 | 0.025 | |
| Sulfur: | Heat analysis | 0.025 | 0.025 | 0.025 | 0.025 |
| Product analysis | 0.025 | 0.025 | 0.025 | 0.025 | |
| Silicon: | Heat analysis | 0.15-0.40 | 0.50-0.80 | 0.50 max | 0.50 max |
| Product analysis | 0.13-0.45 | 0.44-0.86 | 0.50 max | 0.50 max | |
| Chromium: | Heat analysis | 0.80-1.15 | 1.00-1.50 | 2.00-2.50 | 2.00-2.50 |
| Product analysis | 0.74-1.21 | 0.94-1.56 | 1.88-2.62 | 1.88-2.62 | |
| Molybdenum: | Heat analysis | 0.45-0.60 | 0.45-0.65 | 0.90-1.10 | 0.90-1.10 |
| Product analysis | 0.40-0.65 | 0.40-0.70 | 0.85-1.15 | 0.85-1.15 |
Mechanical Properties
- Table 2: For A387 Class 1 Chrome Alloy Steel Plates:
| Tensile Requirements for Class 1 Plates | Grade 2 and 12 | Grade 11 | Grade 22, 21, 5, 9, 21L, 22L |
|---|---|---|---|
| Tensile strength, ksi [MPa] | 55 to 80 [380 to 550] | 60 to 85 [415 to 585] | 60 to 85 [415 to 585] |
| Yield strength, min, ksi [MPa] | 33 [230] | 35 [240] | 30 [205] |
| Elongation in 8 in. [200 mm], min, %A | 18 | 19 | ... |
| Elongation in 2 in. [50 mm], min, %A | 22 | 22 | 18 |
| Reduction of area, min, | ... | ... | 45C40C |
- Table 3: For A387 Class 2 Alloy Steel Plates:
| ensile Requirements for Class 2 Plates<sup>A</sup> | Grade 2 | Grade 11 | Grade 12 | Grades 22, 21, 5, 9 | Grade 91 |
|---|---|---|---|---|---|
| Tensile strength, ksi [MPa] | 70 to 90 [485 to 620] | 75 to 100 [515 to 690] | 65 to 85 [450 to 585] | 75 to 100 [515 to 690] | 85 to 110 [585 to 760] |
| Yield strength, min, ksi [MPa] | 45 [310] | 45 [310] | 40 [275] | 45 [310] | 60 [415] |
| Elongation in 8 in. [200 mm], min, %A | 18 | 18 | 19 | ... | ... |
| Elongation in 2 in. [50 mm], min, %A | 22 | 22 | 22 | 18 | 18 |
| Reduction of area, min, | ... | ... | ... | 45<sup>C</sup>45<sup>D</sup> | ... |
If you want to learn more about GNEE's products, you can send an email to alloy@gneesteelgroup.com. We are more than happy to assist you.



FAQ
Q: What is A387 Grade 11 material?
A: The ASTM A387 specification is the Standard Specification for Pressure Vessel Plates, Alloy Steel, Chromium-Molybdenum intended primarily for use in welded boilers and pressure vessels designed for elevated temperature service.
Q: What is SA 387 GR 11 Cl 1 equivalent material?
A: Sa 387 Gr 11 Equivalent Material
With similar chromium, molybdenum, and chemical content the, Sa 387 Gr 11 Cl 1 Equivalent Material of the BS 621B exhibits identical properties.
Q: What temperature is SA 387 GR 11?
A: In the lower end of the temperature range SA 387 Gr 11 (1150 °F min tempering temperature) , and SA 387 Gr 22 (1250 °F min tempering temperature) are used. These grades can be specified in either class 1 or 2 and can also be provided in the Normalized & Tempered or Quenched and Tempered.
Q: What is the difference between SA 387 GR 11 cl1 and cl2?
A: The difference between SA 387 Grade 11 Class 1 and Class 2 Plate lies in their mechanical properties. However, they both have the same chemical composition. The tensile strength and yield strength of class 2 material is higher than that of class 1, whereas the elongation for class 1 is higher compared to class 2.
Q: What is SA 387 Grade 11 material?
A: Composition: ASME SA387 Grade 11 typically contains about 1% chromium and 0.5% molybdenum. This composition provides good strength and resistance to oxidation at high temperatures. Mechanical Properties: Yield Strength: Minimum of 205 MPa (30,000 psi)
Q: What is the difference between SA 387 Grade 11 CL 1 and Class 2?
A: The Chemical Composition remains the same in both Class 1 and Class 2 (Cl1 and Cl2) but the only Difference is in the Mechanical Properties which is mentioned in below Table.
Q: What is SA 387 Grade 11 Class 2 equivalent to?
A: Sa 387 Gr 11 Equivalent Material is the ASME SA387 in the US markets with the European Union having modules in 13CrMoSi5-5 grade. The Sa 387 Gr 11 Cl 2 Equivalent Material is the SA387-11-2 of the ASME and ASTM standard.
Q: What temperature is SA 387 GR 11?
A: In the lower end of the temperature range SA 387 Gr 11 (1150 °F min tempering temperature) , and SA 387 Gr 22 (1250 °F min tempering temperature) are used. These grades can be specified in either class 1 or 2 and can also be provided in the Normalized & Tempered or Quenched and Tempered.
Q: What is the chemical composition of ASTM A387 Grade 11 Class 2?
A: ASTM A387 GR 11 CL 2 Plates is designed with the composition of chemicals such as carbon, silicon, phosphorous, chromium, sulfur, molybdenum, and manganese. Alloy ASTM A387 is made with specifications such as different standards, finishing, hardness, form, width, and thickness.
Q: What is the difference between SA 516 GR 70 and SA 387 GR 11?
A: Compared to carbon steel plates, SA 387 Gr 11 plates offer superior corrosion and oxidation resistance while maintaining good tensile and yield strength. Compared to SA 516 Gr 70 plates, SA 387 Gr 11 plates have better resistance to oxidation and corrosion, making them a better choice for high-temperature environments.
| Grades Of Pressure Vessel Plates Supplied By GNEE | |||||
| ASTM | ASTM A202/A202M | ASTM A202 Grade A | ASTM A202 Grade B | ||
| ASTM A203/A203M | ASTM A203 Grade A | ASTM A203 Grade B | ASTM A203 Grade D | ASTM A203 Grade E | |
| ASTM A203 Grade F | |||||
| ASTM A204/A204M | ASTM A204 Grade A | ASTM A204 Grade B | ASTM A204 Grade C | ||
| ASTM A285/A285M | ASTM A285 Grade A | ASTM A285 Grade B | ASTM A285 Grade C | ||
| ASTM A299/A299M | ASTM A299 Grade A | ASTM A299 Grade B | |||
| ASTM A302/A302M | ASTM A302 Grade A | ASTM A302 Grade B | ASTM A302 Grade C | ASTM A302 Grade D | |
| ASTM A387/A387M | ASTM A387 Grade 5 Class1 | ASTM A387 Grade 5 Class2 | ASTM A387 Grade 11 Class1 | ASTM A387 Grade 11 Class2 | |
| ASTM A387 Grade 12 Class1 | ASTM A387 Grade 12 Class2 | ASTM A387 Grade 22 Class1 | ASTM A387 Grade 22 Class2 | ||
| ASTM A515/A515M | ASTM A515 Grade 60 | ASTM A515 Grade 65 | ASTM A515 Grade 70 | ||
| ASTM A516/A516M | ASTM A516 Grade 55 | ASTM A516 Grade 60 | ASTM A516 Grade 65 | ASTM A516 Grade 70 | |
| ASTM A517/A517M | ASTM A517 Grade A | ASTM A517 Grade B | ASTM A517 Grade E | ASTM A517 Grade F | |
| ASTM A517 Grade P | ASTM A517 Grade J | ||||
| ASTM A533/A533M | ASTM A533 Grade A Class1 | ASTM A533 Grade B Class1 | ASTM A533 Grade C Class1 | ASTM A533 Grade D Class1 | |
| ASTM A533 Grade A Class2 | ASTM A533 Grade B Class2 | ASTM A533 Grade C Class2 | ASTM A533 Grade D Class2 | ||
| ASTM A533 Grade A Class3 | ASTM A533 Grade B Class3 | ASTM A533 Grade C Class3 | ASTM A533 Grade D Class3 | ||
| ASTM A537/A537M | ASTM A537 Class1 | ASTM A537 Class2 | ASTM A537 Class3 | ||
| ASTM A612/A612M | ASTM A612 | ||||
| ASTM A662/A662M | ASTM A662 Grade A | ASTM A662 Grade B | ASTM A662 Grade C | ||
| EN | EN10028-2 | EN10028-2 P235GH | EN10028-2 P265GH | EN10028-2 P295GH | EN10028-2 P355GH |
| EN10028-2 16MO3 | |||||
| EN10028-3 | EN10028-3 P275N | EN10028-3 P275NH | EN10028-3 P275NL1 | EN10028-3 P275NL2 | |
| EN10028-3 P355N | EN10028-3 P355NH | EN10028-3 P355NL1 | EN10028-3 P355NL2 | ||
| EN10028-3 P460N | EN10028-3 P460NH | EN10028-3 P460NL1 | EN10028-3 P460NL2 | ||
| EN10028-5 | EN10028-5 P355M | EN10028-5 P355ML1 | EN10028-5 P355ML2 | EN10028-5 P420M | |
| EN10028-5 P420ML1 | EN10028-5 P420ML2 | EN10028-5 P460M | EN10028-5 P460ML1 | ||
| EN10028-5 P460ML2 | |||||
| EN10028-6 | EN10028-6 P355Q | EN10028-6 P460Q | EN10028-6 P500Q | EN10028-6 P690Q | |
| EN10028-6 P355QH | EN10028-6 P460QH | EN10028-6 P500QH | EN10028-6 P690QH | ||
| EN10028-6 P355QL1 | EN10028-6 P460QL1 | EN10028-6 P500QL1 | EN10028-6 P690QL1 | ||
| EN10028-6 P355QL2 | EN10028-6 P460QL2 | EN10028-6 P500QL2 | EN10028-6 P690QL2 | ||
| JIS | JIS G3115 | JIS G3115 SPV235 | JIS G3115 SPV315 | JIS G3115 SPV355 | JIS G3115 SPV410 |
| JIS G3115 SPV450 | JIS G3115 SPV490 | ||||
| JIS G3103 | JIS G3103 SB410 | JIS G3103 SB450 | JIS G3103 SB480 | JIS G3103 SB450M | |
| JIS G3103 SB480M | |||||
| GB | GB713 | GB713 Q245R | GB713 Q345R | GB713 Q370R | GB713 12Cr1MoVR |
| GB713 12Cr2Mo1R | GB713 13MnNiMoR | GB713 14Cr1MoR | GB713 15CrMoR | ||
| GB713 18MnMoNbR | |||||
| GB3531 | GB3531 09MnNiDR | GB3531 15MnNiDR | GB3531 16MnDR | ||
| DIN | DIN 17155 | DIN 17155 HI | DIN 17155 HII | DIN 17155 10CrMo910 | DIN 17155 13CrMo44 |
| DIN 17155 15Mo3 | DIN 17155 17Mn4 | DIN 17155 19Mn6 | |||