A36 steel is a common structural steel alloy utilized in the United States.The A36 (UNS K02600) standard was established by the ASTM International. The standard was published in 1960 and has been updated several times since. Prior to 1960, the dominant standards for structural steel in North America were A7 (until 1967) and A9 (for buildings, until 1940). Note that SAE/AISI A7 and A9 tool steels are not the same as the obsolete ASTM A7 and A9 structural steels.

| Chemical composition (%, ≤) for shapes | ||||||
| Standard | C | Si | Mn | P | S | Cu |
| ASTM A36/A36M | 0.26 | 0.40 | 1.03 | 0.04 | 0.05 | 0.20 |
Note: For shapes with a flange thickness more than 3 in (76 mm), 0.85-1.35% manganese content and 0.15-0.40% silicon content are required.

As with most steels, A36 has a density of 7,800 kg/m3 (0.28 lb/cu in). Young's modulus for A36 steel is 200 GPa. A36 steel has a Poisson's ratio of 0.32 and a shear modulus of 78 GPa (11,300,000 psi).
A36 steel in plates, bars, and shapes with a thickness of less than 8 in (203 mm) has a minimum yield strength of 36,000 psi (250 MPa) and ultimate tensile strength of 58,000–80,000 psi (400–550 MPa). Plates thicker than 8 in have a 32,000 psi (220 MPa) yield strength and the same ultimate tensile strength of 58,000–80,000 psi (400–550 MPa).The electrical resistance of A36 is 0.142 μΩm at 20 °C. A36 bars and shapes maintain their ultimate strength up to 650 °F (343 °C). Afterward, the minimum strength drops off from 58,000 psi (400 MPa): 54,000 psi (370 MPa) at 700 °F (371 °C); 45,000 psi (310 MPa) at 750 °F (399 °C); 37,000 psi (260 MPa) at 800 °F (427 °C).