A387Gr22CL1 is a chromium-molybdenum alloy steel plate in the ASTM A387 standard with a higher grade than Gr11, characterized by significantly enhanced alloying elements. "Gr22" indicates that its chromium (Cr) content is increased to approximately 2.00%-2.50%, while molybdenum (Mo) content is maintained at around 0.90%-1.10%. The doubled chromium content brings a qualitative leap, making its oxidation resistance and corrosion resistance-especially resistance to high-temperature hydrogen sulfide corrosion-far superior to Gr11. The substantial increase in molybdenum content greatly enhances the steel's high-temperature strength, creep resistance, and microstructural stability. Therefore, Gr22CL1 is positioned to cope with more severe medium-temperature and high-pressure environments. Its upper limit of service temperature is usually 25-50°C higher than that of Gr11, enabling long-term stable operation in the temperature range of 454°C to 566°C. It is a key material for manufacturing heavy-duty pressure vessels.
Analysis of High-Temperature Strength and Creep Resistance of A387Gr22CL1 Steel Plate
The core advantage of Gr22CL1 lies in its excellent high-temperature creep rupture strength. Creep refers to the slow plastic deformation of materials under continuous high temperature and stress, which is a major constraint in the design of high-temperature equipment. The higher molybdenum content and more stable alloy carbides (such as M7C3, M2C) formed by the combined action of chromium and molybdenum can effectively pin grain boundaries and hinder dislocation movement, thereby significantly improving the material's creep limit and creep rupture strength limit. This means that under the same design temperature and pressure, using Gr22CL1 can design lighter and thinner equipment compared to lower-grade materials (such as Gr11), achieving weight reduction and material savings. Alternatively, with the same wall thickness, Gr22CL1 equipment can withstand higher operating pressure and temperature, meeting more advanced process requirements-for example, applications in coal liquefaction and modern hydrocracking units.
Microstructural Stability and Temper Embrittlement Phenomenon of A387Gr22CL1 Steel Plate
After heat treatment (usually normalizing + tempering), Gr22CL1 steel plate obtains a stable tempered bainite structure. However, unlike low-alloy steels, high chromium-molybdenum steels (such as 2.25Cr-1Mo steel) have a characteristic that requires special attention-temper embrittlement. This refers to the phenomenon where the impact toughness of the steel decreases significantly when serving for a long time in the temperature range of 375°C to 575°C or cooling slowly through this range. It is not a corrosion problem but is caused by the segregation of impurity elements (such as phosphorus, tin, antimony) at grain boundaries.
Therefore, for Gr22CL1 material, in addition to strictly controlling the content of impurity elements in the steel (producing high-purity steel plates using refining technologies such as vacuum degassing), the Post-Weld Heat Treatment (PWHT) during manufacturing must strictly control the heating/cooling rate to avoid prolonged stay in the embrittlement temperature range. At the same time, its toughness evaluation must be based on test plates subjected to simulated post-weld heat treatment to ensure that the material still has sufficient toughness in the final state after equipment manufacturing.
Irreplaceability of A387Gr22CL1 Steel Plate in Extreme Process Environments
Due to its comprehensive performance, Gr22CL1 steel plate has become a "standard" material for many modern high-end energy and chemical process equipment.
It is widely used in:
1. Large-capacity, high-severity hydroprocessing reactors: especially heavy oil hydrocracking and residue hydrotreating reactors, which operate at higher pressure, handle heavier media, and have stronger corrosion.
2. Core coal chemical equipment: such as coal liquefaction reactors, high-pressure waste heat boilers and shift converters of large-scale high-efficiency coal gasification units, which face high temperature, high pressure, high hydrogen partial pressure, and syngas corrosion.
3. Large-thickness high-pressure vessels: Due to Gr22's higher strength, when manufacturing ultra-thick-walled vessels (such as certain equipment in nuclear power and chemical fields), it can effectively reduce wall thickness and solve the difficulties in smelting, forging, heat treatment, and welding caused by large thickness.
In these fields, the performance of Gr11 can no longer meet the requirements, and Gr22CL1 has become the foundation for ensuring the safe, stable, long-term, full-load, and efficient operation of the equipment.
Strict Manufacturing and Welding Process Challenges of A387Gr22CL1 Steel Plate
Selecting Gr22CL1 means accepting more complex manufacturing process challenges. Its weldability is more sensitive than that of Gr11. Higher-grade welding materials must be used, such as AWS A5.5 E9018-B3L ("B3" corresponds to Gr22, "L" indicates low-temperature toughness).
The preheating temperature and interpass temperature control need to be stricter (usually requiring not less than 200°C).
The most critical link is Post-Weld Heat Treatment (PWHT), whose specifications are extremely strict: the heat treatment temperature must be higher than the maximum service temperature of the material, usually in the range of 690°C ± 14°C; the holding time must be accurately calculated to ensure sufficient stress relief without causing excessive softening; the heating and cooling rates must be controlled to avoid the temper embrittlement zone and prevent the generation of new stresses. Any process deviation may lead to unqualified joint performance and even early failure during service.
Technological Evolution of A387Gr22CL1 Steel Plate and Comparison with Higher-Grade Materials
Gr22CL1 is a classic grade that connects the past and the future in the chromium-molybdenum steel family. With technological progress, to pursue higher efficiency, improved types (such as Gr22Cl.2, Gr24) adding trace elements like vanadium (V) and niobium (Nb) based on Gr22 have emerged, featuring better high-temperature strength.
In addition, to completely solve the problem of temper embrittlement, high-purity Gr22 with low impurity content (such as SA-542 Type D) has been developed. Gr22CL1 and these new materials together form a technical sequence.
When selecting, a comprehensive technical and economic evaluation is required: for most traditional large-scale hydroprocessing reactors, Gr22CL1-with mature technology and rich application experience-is still one of the most cost-effective choices. For equipment with ultra-high temperature, ultra-long design life, or extreme toughness requirements, more advanced improved models can be considered. Understanding the performance boundaries of Gr22CL1 is a prerequisite for scientific material selection and advanced equipment design.
If you want to learn more about GNEE's products, you can send an email to alloy@gneesteelgroup.com. We are more than happy to assist you.
FAQ
Q: What is ASTM A387 material?
A: The ASTM A387 specification is the Standard Specification for Pressure Vessel Plates, Alloy Steel, Chromium-Molybdenum plates used in the application of welded boilers and pressure vessels subjected to elevated temperatures. The two grades SSAB produces are available as Class 1 and/or Class 2.
Q: What is the chemical composition of ASTM A387 Grade 22?
A: ASTM A387 GR 22 CL 2 Plates is designed with chemical compositions like carbon, manganese, phosphorus, molybdenum, chromium, silicon, and sulfur. This A387 alloy is constructed with various classifications like area reduction, elongation, yield strength, and high tensile strength.
Q: What is SA 387 22 material?
A: What is SA 387 Grade 22? ASME SA387-22 steel plate is a pressure vessel grade steel specially designed for use in elevated temperature service and applications in which sour gas is present.
Q: What is the hardness of SA 387 GR 22 cl2?
A: Tensile Strength: 75 ksi - 100 ksi (515 MPa - 690 MPa) Yield Strength: 40 ksi (275 MPa) minimum. Elongation: 20% minimum in 2 inches. Hardness: Typically between 130 and 170 HB.
Q: What is A387 GR 22 equivalent to?
A: Among the ASTM A387 Grade 22 equivalent steel grades, SA387 Grade 22, 10CrMo9-10 is more popular than other equivalents. SA387 Grade 22 steel is under ASME SA387/ SA387M standard. The chemical performance and technical requirements of SA387 Grade 22 steel is almost same with ASTM A387 Grade 22 steel.
Q: What is the difference between SA 387 Grade 11 CL 1 and Class 2?
A: The difference between SA 387 Grade 11 Class 1 and Class 2 Plate lies in their mechanical properties. However, they both have the same chemical composition. The tensile strength and yield strength of class 2 material is higher than that of class 1, whereas the elongation for class 1 is higher compared to class 2.
Q: What is the ASTM A387 Grade 11 equivalent to?
A: Sa 387 Gr 11 Equivalent Material
The Sa 387 Gr 11 Cl 2 Equivalent Material is the SA387-11-2 of the ASME and ASTM standard. With similar chromium, molybdenum, and chemical content the, Sa 387 Gr 11 Cl 1 Equivalent Material of the BS 621B exhibits identical properties.
| Grades Of Pressure Vessel Plates Supplied By GNEE | |||||
| ASTM | ASTM A202/A202M | ASTM A202 Grade A | ASTM A202 Grade B | ||
| ASTM A203/A203M | ASTM A203 Grade A | ASTM A203 Grade B | ASTM A203 Grade D | ASTM A203 Grade E | |
| ASTM A203 Grade F | |||||
| ASTM A204/A204M | ASTM A204 Grade A | ASTM A204 Grade B | ASTM A204 Grade C | ||
| ASTM A285/A285M | ASTM A285 Grade A | ASTM A285 Grade B | ASTM A285 Grade C | ||
| ASTM A299/A299M | ASTM A299 Grade A | ASTM A299 Grade B | |||
| ASTM A302/A302M | ASTM A302 Grade A | ASTM A302 Grade B | ASTM A302 Grade C | ASTM A302 Grade D | |
| ASTM A387/A387M | ASTM A387 Grade 5 Class1 | ASTM A387 Grade 5 Class2 | ASTM A387 Grade 11 Class1 | ASTM A387 Grade 11 Class2 | |
| ASTM A387 Grade 12 Class1 | ASTM A387 Grade 12 Class2 | ASTM A387 Grade 22 Class1 | ASTM A387 Grade 22 Class2 | ||
| ASTM A515/A515M | ASTM A515 Grade 60 | ASTM A515 Grade 65 | ASTM A515 Grade 70 | ||
| ASTM A516/A516M | ASTM A516 Grade 55 | ASTM A516 Grade 60 | ASTM A516 Grade 65 | ASTM A516 Grade 70 | |
| ASTM A517/A517M | ASTM A517 Grade A | ASTM A517 Grade B | ASTM A517 Grade E | ASTM A517 Grade F | |
| ASTM A517 Grade P | ASTM A517 Grade J | ||||
| ASTM A533/A533M | ASTM A533 Grade A Class1 | ASTM A533 Grade B Class1 | ASTM A533 Grade C Class1 | ASTM A533 Grade D Class1 | |
| ASTM A533 Grade A Class2 | ASTM A533 Grade B Class2 | ASTM A533 Grade C Class2 | ASTM A533 Grade D Class2 | ||
| ASTM A533 Grade A Class3 | ASTM A533 Grade B Class3 | ASTM A533 Grade C Class3 | ASTM A533 Grade D Class3 | ||
| ASTM A537/A537M | ASTM A537 Class1 | ASTM A537 Class2 | ASTM A537 Class3 | ||
| ASTM A612/A612M | ASTM A612 | ||||
| ASTM A662/A662M | ASTM A662 Grade A | ASTM A662 Grade B | ASTM A662 Grade C | ||
| EN | EN10028-2 | EN10028-2 P235GH | EN10028-2 P265GH | EN10028-2 P295GH | EN10028-2 P355GH |
| EN10028-2 16MO3 | |||||
| EN10028-3 | EN10028-3 P275N | EN10028-3 P275NH | EN10028-3 P275NL1 | EN10028-3 P275NL2 | |
| EN10028-3 P355N | EN10028-3 P355NH | EN10028-3 P355NL1 | EN10028-3 P355NL2 | ||
| EN10028-3 P460N | EN10028-3 P460NH | EN10028-3 P460NL1 | EN10028-3 P460NL2 | ||
| EN10028-5 | EN10028-5 P355M | EN10028-5 P355ML1 | EN10028-5 P355ML2 | EN10028-5 P420M | |
| EN10028-5 P420ML1 | EN10028-5 P420ML2 | EN10028-5 P460M | EN10028-5 P460ML1 | ||
| EN10028-5 P460ML2 | |||||
| EN10028-6 | EN10028-6 P355Q | EN10028-6 P460Q | EN10028-6 P500Q | EN10028-6 P690Q | |
| EN10028-6 P355QH | EN10028-6 P460QH | EN10028-6 P500QH | EN10028-6 P690QH | ||
| EN10028-6 P355QL1 | EN10028-6 P460QL1 | EN10028-6 P500QL1 | EN10028-6 P690QL1 | ||
| EN10028-6 P355QL2 | EN10028-6 P460QL2 | EN10028-6 P500QL2 | EN10028-6 P690QL2 | ||
| JIS | JIS G3115 | JIS G3115 SPV235 | JIS G3115 SPV315 | JIS G3115 SPV355 | JIS G3115 SPV410 |
| JIS G3115 SPV450 | JIS G3115 SPV490 | ||||
| JIS G3103 | JIS G3103 SB410 | JIS G3103 SB450 | JIS G3103 SB480 | JIS G3103 SB450M | |
| JIS G3103 SB480M | |||||
| GB | GB713 | GB713 Q245R | GB713 Q345R | GB713 Q370R | GB713 12Cr1MoVR |
| GB713 12Cr2Mo1R | GB713 13MnNiMoR | GB713 14Cr1MoR | GB713 15CrMoR | ||
| GB713 18MnMoNbR | |||||
| GB3531 | GB3531 09MnNiDR | GB3531 15MnNiDR | GB3531 16MnDR | ||
| DIN | DIN 17155 | DIN 17155 HI | DIN 17155 HII | DIN 17155 10CrMo910 | DIN 17155 13CrMo44 |
| DIN 17155 15Mo3 | DIN 17155 17Mn4 | DIN 17155 19Mn6 | |||