What is the difference between S275J2 and S355J2 ?

Jul 08, 2025 Leave a message

S355J2-N-MTC-steel-plate.pdf

What is the grade S275J2 (1.0145)?

Grade S275J2 has a minimum yield strength of 275 MPa. The impact energy at a test temperature of -20°C is at least 27 joules.

 

What is the difference between S275J2 and S355J2 ?

S355JR VS S355J2:has better toughness as it is tested at -20°C compared to S355JR, which is tested at 20°C.
S355J2 vs. S275J2:S355J2 has a higher strength (355 MPa) compared to S275J2 (275 MPa).

 

Chemical Composition of Structural Steels - S235, S275 and S355

Grade C% Mn% P% S% Si%
S235 0.22 max 1.60 max 0.05 max 0.05 max 0.05 max
S275 0.25 max 1.60 max 0.04 max 0.05 max 0.05 max
S355 0.23 max 1.60 max 0.05 max 0.05 max 0.05 max

 

Yield Strength of of Structural Steel - S235, S275, S355

Structural Steel Grade at 16mm Minimum Yield Strength at nominal thickness 16mm
ksi N/mm 2 (MPa)
S235 33 000 ksi 235 N/mm 2
S275 36 000 ksi 275 N/mm 2
S355 50 000 ksi 355 N/mm 2

 

Tensile Strength of of Structural Steel - S235, S275, S355

Structural Steel Grade Tensile Strength MPa at Nom thickness between 3mm and 16mm
S235 360 – 510 MPa
S275 370 – 530 MPa
S355 470 – 630 MPa

 

What is the difference between 275jr and 275j2?
The main difference among the three S275 steel lies in their impact temperature: 20℃ of S275JR steel, -20℃ of S275J2 steel and 0℃ of S275J0 steel.

 

S275J2 (1.0145) equivalent China standard

Q275D

The China standard equivalent to the European steel grade S275J2 is GB/T 1591-2018 Q275D. S275J2, according to EN 10025-2, is a non-alloy structural steel with a minimum yield strength of 275 MPa. The Chinese standard Q275, found in GB/T 700, is also a structural steel with similar properties.

EU
EN
England
BS
European old
EN
Belgium
NBN
China
GB/T 1591-2018
Sweden
SS
India
IS
S275J2 (1.0145)
43EE
Fe430D2
S275J2G4
AE295DD
Q275D
1414-01
Fe410WC

 

S275  equivalent