What is SPA-H 1.8945 S355J0WP High strength weathering steel plate?
SPA H Steel, also known as weathering steel, is a high-strength low-alloy steel that exhibits excellent resistance to atmospheric corrosion. It is classified as a low-alloy structural steel, primarily alloyed with copper, chromium, and nickel, which contribute to its unique properties. The primary alloying elements in SPA H Steel enhance its durability and weather resistance, allowing it to develop a protective patina when exposed to the elements. This patina forms a barrier that slows down further corrosion, making it particularly suitable for outdoor applications.
SPA-H steel is a high-strength, low-alloy weathering steel that conforms to the Japanese industrial standard JIS G3125. It is designed to be highly resistant to atmospheric corrosion by forming a stable, protective rust-like layer on its surface when exposed to the elements. This property makes it suitable for applications like bridge construction, railway carriages, and shipping containers where long-term durability in outdoor conditions is essential.
SPA-H Corten steel widely used in air preheater, economizer, railway carriage, containers production, bridge building , construction and so on.
SPA-H (JIS ) - Worldwide equivalent grades
Worldwide equivalents of grade SPA-H (Japan: JIS )
| Steel : SPA-H | Japan | Standard : JIS |
Cross reference table
for Steel SPA-H (JIS ) and its European equivalent S355J0WP (1.8945) ( EN )
| EU EN |
USA - |
Germany DIN,WNr |
Japan JIS |
France AFNOR |
England BS |
European old EN |
Italy UNI |
China GB |
Poland PN |
Czechia CSN |
Inter ISO |
||||||||||||||
| S355J0WP (1.8945) |
|
|
|
|
|
|
|
|
|
|
|
Alternative Names, Standards, and Equivalents
| Standard Organization | Designation/Grade | Country/Region of Origin | Notes/Remarks |
|---|---|---|---|
| UNS | K12043 | USA | Closest equivalent to ASTM A588 |
| ASTM | A588 | USA | Weathering steel standard |
| EN | S355J0W | Europe | Minor compositional differences |
| JIS | G3125 | Japan | Similar properties, used in Japanese applications |
| GB | Q345GNH | China | Comparable weathering steel grade |
The differences between these grades often lie in specific alloying elements and mechanical properties, which can affect performance in particular applications. For instance, while ASTM A588 and SPA H Steel are similar, the former may have slightly different yield strength requirements.
SPA-H Weathering steel Technical Data

SPA-H Weathering steel chemical composition
| Grade | C ≤ | Si | Mn | P | S ≤ | Cu | Cr | Ni ≤ |
| SPA-H | 0.12 | 0.25~0.75 | 0.20~0.50 | 0.070~0.150 | 0.040 | 0.25~0.60 | 0.30~1.25 | 0.65 |
SPA-H Weathering resistant steel tensile property request
| Grade | Plate Thickness | Yield strength | Tensile strength | elongation |
| SPA-H | ≤ 6.0mm | ≥ 345 MPa | ≥ 480 MPa | ≥ 22 |
| > 6.0mm | ≥ 335 MPa | ≥ 490 MPa | ≥ 15 |
SPA-H steel delivery condition can be hot rolled, Cold rolled ,AR/CR/N/TMCP/T/QT as the customer request
Relate Steel Type
| Steel Type | Standard | Country Code | C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Cu(%) |
| SPA-H | 4620 | CNS | ≦0.12 | 0.25-0.75 | 0.20-0.50 | 0.07-0.15 | ≦0.04 | 0.30-1.25 | 0.25-0.60 |
| SPA-H | G3125 | JIS | ≦0.12 | 0.25-0.75 | 0.20-0.50 | 0.07-0.15 | ≦0.04 | 0.30-1.25 | 0.25-0.60 |
| Type1 | A242 | ASTM | ≦0.15 | ≦1.00 | ≦0.15 | ≦0.05 | ≧0.20 |
| Steel Type | Yield stress (Mpa) | Tensile stress (Mpa) | Elongation (%) | Thick (mm) |
| SPA-H | ≧345 | ≧480 | ≧22 | ≦6.0 |
| SPA-H | ≧345 | ≧480 | ≧22 | ≦6.0 |
| Type1 | ≧345 | ≧480 | ≧21 | ≦20.0 |
Advantages of SPA H Steel:
- Corrosion Resistance: The formation of a protective oxide layer reduces maintenance costs and extends the lifespan of structures.
- High Strength: Offers excellent mechanical properties, allowing for thinner sections and reduced weight in structural applications.
- Aesthetic Appeal: The unique weathered appearance is often desirable in architectural applications.
Limitations of SPA H Steel:
- Initial Cost: Higher initial material costs compared to conventional carbon steels.
- Limited Ductility: While strong, it may not perform as well in applications requiring extensive deformation.
- Welding Considerations: Requires careful selection of filler materials and welding techniques to avoid issues such as cracking.
Historically, SPA H Steel has gained popularity in construction and infrastructure projects due to its longevity and reduced maintenance needs, positioning it as a preferred choice in the market.
SPA-H Steel Heat Resistance
| Property/Limit | Temperature (°C) | Temperature (°F) | Remarks |
|---|---|---|---|
| Max Continuous Service Temp | 400 °C | 752 °F | Suitable for structural applications |
| Max Intermittent Service Temp | 450 °C | 842 °F | Short-term exposure only |
| Scaling Temperature | 500 °C | 932 °F | Risk of oxidation at high temps |
SPA H Steel maintains its mechanical properties at elevated temperatures, making it suitable for applications where thermal exposure is a concern. However, prolonged exposure to temperatures above 400 °C can lead to scaling and reduced mechanical performance.
SPA-H Fabrication Properties
Weldability
| Welding Process | Recommended Filler Metal (AWS Classification) | Typical Shielding Gas/Flux | Notes |
|---|---|---|---|
| SMAW | E7018 | Argon + CO2 | Preheat recommended |
| GMAW | ER70S-6 | Argon + CO2 | Post-weld heat treatment may be required |
SPA H Steel is generally weldable using standard techniques, but care must be taken to select appropriate filler materials to avoid cracking. Preheating before welding can help mitigate the risk of defects, and post-weld heat treatment can enhance the overall performance of the weld.
Machinability
| Machining Parameter | SPA H Steel | AISI 1212 | Notes/Tips |
|---|---|---|---|
| Relative Machinability Index | 60 | 100 | Moderate machinability |
| Typical Cutting Speed | 25 m/min | 40 m/min | Adjust tooling for better performance |
SPA H Steel has moderate machinability compared to benchmark steels. Optimal cutting speeds and tooling must be selected to achieve desired surface finishes and tolerances.
Formability
SPA H Steel exhibits good formability in both cold and hot working processes. However, it is essential to consider the work hardening characteristics, as excessive deformation can lead to increased strength but reduced ductility. Recommended bend radii should be adhered to in order to prevent cracking during forming operations.
4.4 Heat Treatment
| Treatment Process | Temperature Range (°C/°F) | Typical Soaking Time | Cooling Method | Primary Purpose / Expected Result |
|---|---|---|---|---|
| Annealing | 600 - 700 °C / 1112 - 1292 °F | 1 - 2 hours | Air cooling | Softening, improved ductility |
| Normalizing | 900 - 950 °C / 1652 - 1742 °F | 1 - 2 hours | Air cooling | Refined grain structure |
Heat treatment processes such as annealing and normalizing can significantly alter the microstructure of SPA H Steel, enhancing its mechanical properties and making it suitable for various applications. The transformation during these treatments can lead to improved toughness and ductility, which are critical for structural integrity.
Typical Applications and End Uses
| Industry/Sector | Specific Application Example | Key Steel Properties Utilized in this Application | Reason for Selection |
|---|---|---|---|
| Construction | Bridges | High strength, corrosion resistance | Long lifespan, reduced maintenance |
| Architecture | Sculptures | Aesthetic appeal, weather resistance | Unique appearance, durability |
| Transportation | Railcars | High strength, toughness | Safety and reliability |
| Energy | Wind Turbine Towers | Corrosion resistance, structural integrity | Longevity in harsh environments |
Other applications include:
- Outdoor sculptures and art installations
- Storage tanks and silos
- Retaining walls and landscaping features
SPA H Steel is chosen for these applications due to its ability to withstand environmental challenges while maintaining structural integrity and aesthetic appeal.
Important Considerations, Selection Criteria, and Further Insights
| Feature/Property | SPA H Steel | ASTM A588 | S355J0W | Brief Pro/Con or Trade-off Note |
|---|---|---|---|---|
| Key Mechanical Property | High strength | High strength | Moderate strength | SPA H offers superior corrosion resistance |
| Key Corrosion Aspect | Excellent | Excellent | Good | SPA H performs better in urban environments |
| Weldability | Good | Good | Moderate | SPA H requires careful filler selection |
| Machinability | Moderate | Good | Good | SPA H is less machinable than A588 |
| Formability | Good | Good | Moderate | SPA H has better formability characteristics |
| Approx. Relative Cost | Moderate | Moderate | Low | Cost may vary based on market conditions |
| Typical Availability | Moderate | High | High | Availability can affect project timelines |
When selecting SPA H Steel, considerations such as cost-effectiveness, availability, and specific application requirements must be evaluated. The unique properties of SPA H Steel make it suitable for a variety of applications, particularly where corrosion resistance and aesthetic appeal are paramount. Additionally, its performance in harsh environments makes it a reliable choice for long-term structural applications.
What's the difference between Corten A and SPA-H Corten steel?
| Chemical Composition (%) | |||||||||
| Grade | C | Si | Mn | P | S | Cr | Cu | V | Ni |
| Corten A | 0.12 | 0.25-0.75 | 0.20-0.50 | 0.07-0.15 | 0.03 | 0.50-1.25 | 0.25-0.55 | – | 0.65 |
| SPA-H | 0.12 | 0.20-0.75 | 0.6 | 0.07-0.15 | 0.035 | 0.30-1.25 | 0.25-0.50 | – | 0.65 |
Mechanical Properties
At room temperature for plates ? 3mm in thickness (transverse test specimens, according to EN 10002).
Requirements to hot rolled plates ? 3mm in thickness according to EN 10025-5.
| Grade | Minimum yield point (ReH Mpa *) | Tensile strength MPa | Minimum elongation A(Lo=5.65 ?So) % |
| Corten A | 355 | 470-630 | 20 |
| SPA-H | 355 | 490 | 22 |