EN10028-3 P275NL2 is a pressure vessel steel grade that is widely used in the fabrication of pressure vessels and boilers due to its excellent mechanical properties and resistance to low-temperature environments. This grade is compliant with the European standard EN10028-3, which specifies requirements for flat products for pressure equipment made of weldable fine-grain steels.
Chemical Composition:
The chemical composition of P275NL2 is carefully controlled to ensure the necessary mechanical properties and weldability. The typical chemical composition includes:
|
P275NL2 Chemical Composition |
|||||||
|
Grade |
The Element Max (%) |
||||||
|
C |
Si |
Mn |
P |
S |
Al(min) |
N |
|
|
P275NL2 |
0.16 |
0.40 |
0.5-1.40 |
0.025 |
0.015 |
|
0.02 |
|
Cr |
Cu |
Mo |
Nb |
Ni |
Ti |
V |
|
|
0.30 |
0.30 |
0.08 |
0.005 |
0.50 |
0.03 |
0.05 |
|
Carbon Equivalent: Ceq = 【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%
Mechanical Properties:
The mechanical properties of P275NL2 are characterized by its high strength and toughness, which are crucial for pressure vessel applications. Typical mechanical properties are as follows:
|
Grade |
|
P275NL2 Mechanical Property |
|||||
|
Thickness |
Yield |
Tensilmie |
Elongation |
Impact Energy(KV J) min |
|||
|
P275NL2 |
mm |
Min Mpa |
Mpa |
Min % |
-20° |
0° |
+20° |
|
≤ 16 |
275 |
390-510 |
24 |
65 |
90 |
100 |
|
|
16> to ≤35 |
275 |
390-510 |
24 |
65 |
90 |
100 |
|
|
35> to ≤50 |
265 |
390-510 |
24 |
65 |
90 |
100 |
|
|
50> to ≤70 |
255 |
390-510 |
24 |
65 |
90 |
100 |
|
|
70> to ≤100 |
235 |
370-490 |
23 |
65 |
90 |
100 |
|
|
100> to ≤150 |
235 |
350-470 |
23 |
65 |
90 |
100 |
|
Heat Treatment:
P275NL2 is generally supplied in a normalized condition. Normalization is a heat treatment process that involves heating the steel to a temperature above its upper critical point and then cooling it in air. This process refines the grain structure and improves the mechanical properties of the steel.
Low-Temperature Impact Test:
The steel grade is subjected to a low-temperature impact test to ensure its suitability for use in low-temperature environments. The impact energy values are measured at -40°C, which is a critical temperature for many applications where the equipment may be exposed to cold conditions.
|
Equivalent steel grade of P275NL2 |
|||||||
|
Europe |
Belgium |
Germany |
BS 1501 |
Italy |
ASTM |
India |
Japan |
|
|
|
ESt E285 |
|
|
|
|
|