ASTM A514 Grade B is a high-strength, quenched, and tempered alloy steel primarily used in structural applications where high yield strength and weldability are critical. It is part of the ASTM A514 specification for high-yield-strength, quenched,d, and tempered alloy steel plate suitable for welding.
Chemical Composition (Typical)
| Grade | C | Mn | P | S | SI | Ni | Cr | Mo | V | Ti | Zr | Cu | B |
| A514GrB | 0.12-0.21 | 0.7-1.0 | ≤0.035 | ≤0.04 | 0.2-0.35 | ~ | 0.4-0.65 | 0.15-0.25 | 0.03-0.08 | 0.01-0.03 | ~ | ~ | 0.0005-0.005 |
Key Mechanical Properties
| Grade | Thickness Inch |
Yield Strength Mpa |
Tensile Strength Mpa |
Elongation in 50mm | Hardnees Brinell |
| A514GrB | less 3/4 inch | 690 | 760-895 | 18 | 235 |
| over 3/4 to 2 1/2 | 690 | 760-895 | 18 | ~ | |
| over 2 1/2 to 6 inch | 620 | 690-895 | 16 | ~ |
Equivalents (Approximate):
Key Features

High Strength-to-Weight Ratio: Ideal for lightweight yet durable structures.
Weldability: Requires preheating (150–230°C / 300–450°F) and post-weld heat treatment (PWHT) to avoid cracking.
Toughness: Excellent impact resistance at low temperatures.
Fatigue Resistance: Suitable for cyclic loading applications.
Machinability: Moderate (requires carbide tools due to hardness).
Applications
Structural Engineering: Bridge components, crane booms, and high-rise building frames.
Heavy Equipment: Excavator arms, bulldozer blades, and mining machinery.
Transportation: Truck frames, trailer chassis, and railcar components.
Military/Aerospace: Armored vehicle parts and load-bearing structures.
Oil & Gas: Offshore platforms and drilling equipment.
Processing Notes
Heat Treatment: Quenched and tempered (Q&T) to achieve optimal strength and toughness.
Thickness: Available in plates up to 6.5 inches (165 mm), though thicker sections may require adjusted heat treatment.
Corrosion Resistance: Not inherently corrosion-resistant; requires coatings (e.g., galvanizing) for outdoor use.
Comparison to Other Grades
- ASTM A572 Grade 50: Lower strength (345 MPa yield) but cheaper for non-critical structures.
- ASTM A36: Mild steel with lower strength (250 MPa yield) but better machinability.
- ASTM A517 (Grade B): Higher strength (760 MPa yield) but more expensive, used in pressure vessels.
Why Choose A514 Grade B?
It balances high strength, weldability, and toughness, making it ideal for applications demanding structural integrity under heavy loads or harsh environments. Always consult ASTM A514 specifications for project-specific requirements.
For more information, please contact me freely.
Email: alloy@gneesteelgroup.com
Whatsapp (WeChat): +86-15824687445
FAQ
Q: What is ASTM A514 grade B?
A: ASTM A514 Grade B is a quenched and tempered alloy steel plate for structural applications requiring high yield strength combined with good formability and toughness. A514 Grade B has a minimum yield strength of 100 ksi [690 MPa] and may be ordered with supplemental Charpy V-notch impact test requirements.
Q: What is A514 grade equivalent to?
A: Other designations that are equivalent to AISI A514 grade F alloy steel include the following: ASTM A514 (F) ASTM A517 (F)
| Other steel plate | ||||
| Name | Material | Specification (mm) | Tons | Remark |
| Low Alloy | Q345A, Q345B, Q345C, Q345D, Q345E, Q390, Q420, Q460C, ST52-3, S355J2+N, SS400, SA302GrC, S275NL, 35CrMo | 6 - 350 | 5788.56 | Normalizing, tempered ,controlled rolling, hot rolling , Hot rolling,1st inspection, 2nd inspection, 3rd inspection |
| Pressure Vessel Plate | Q245R, Q345R, Q370R, 16MnDR, 09MnNiDR, 15CrMoR, 14Cr1MoR, 12Cr2Mo1R, SA516Gr60, SA516Gr70, SA516Gr485, SA285, SA387Gr11, SA387Gr12, SA387Gr22, P265,P295,P355GH,Q245R(R-HIC),Q345R(R-HIC) | 3 - 300 | 8650 | Normalizing, tempered ,controlled rolling, hot rolling , Hot rolling,1st inspection, 2nd inspection, 3rd inspection |
| High-Strength Plate | WH785D/E,Q960D/E, Q890D/E,WH60D/E,WH70B,Q550D,Q590D,Q690D/E | 8 - 120 | 3086.352 | Quenched and tempered |
| Wear-Resistant Plate | NM360, NM400, NM450, NM500 | 6 - 150 | 3866.297 | Quenched and tempered |
| Bridge Plate | Q235qC, Q345qC, Q370qC, Q420qC, Q345qDNH, Q370qDNH, A709 - 50F - 2, A709 - 50T - 2 | 8 - 200 | 2853.621 | Hot rolling, normalized ,hot rolling controlled rolling, quenched and tempered + toughness and brittleness |