What Is 15Mo3 Steel Plate?
15Mo3 is a carbon molybdenum alloy steel plate specified in DIN 17155, the German standard for plates for boilers and pressure vessels that has since been withdrawn. The grade was developed for equipment operating in the elevated temperature range, where plain carbon steel loses creep strength and where hydrogen containing process media require better resistance to hydrogen attack. Modern purchasing documents normally replace the designation with EN 10028-2 16Mo3, which covers the same 0.25 - 0.35 % molybdenum C-Mo steel family, but 15Mo3 still appears on existing equipment records and on drawings prepared before the standard was superseded.
Chemical Composition of 15Mo3
The chemistry is a low carbon, low alloy balance. Molybdenum is the only deliberate alloying addition in significant quantity; it raises creep strength at temperature and improves resistance to hydrogen attack. Phosphorus and sulphur are kept low so that the plate retains toughness in the normalised condition.
| Element | Requirement, % | Purpose |
|---|---|---|
| C | 0.12 - 0.20 | Strength and hardenability control |
| Si | 0.10 - 0.35 | Deoxidation |
| Mn | 0.40 - 0.90 | Strength and toughness |
| P | 0.035 max | Restricted for toughness |
| S | 0.030 max | Restricted for cleanliness |
| Mo | 0.25 - 0.35 | Creep strength, hydrogen resistance |
| Cr | 0.30 max | Residual control |
| Ni | 0.30 max | Residual control |
| Cu | 0.30 max | Residual control |
Mechanical Properties and Thickness Limits
Minimum yield strength is specified against plate thickness, because quench rate and rolling reduction both fall as the section gets heavier. Tensile strength is quoted at 440 - 590 MPa across the normal plate range. Impact testing is carried out on Charpy V-notch specimens, and additional impact temperatures can be ordered where an evaporator, for example, cycles colder than the base specification covers.
| Thickness, mm | ReH min, MPa | Rm, MPa |
|---|---|---|
| 6 - 16 | 275 | 440 - 590 |
| over 16 - 40 | 270 | 440 - 590 |
| over 40 - 60 | 260 | 440 - 590 |
| over 60 - 100 | 240 | 440 - 590 |
| over 100 - 150 | 220 | 440 - 590 |
Delivery Condition and Supplementary Requirements
Plate for boiler and pressure vessel service is normally supplied normalised, which refines the grain structure and stabilises toughness after rolling. As rolled, thermo-mechanically controlled rolled and quenched and tempered conditions are also used for particular applications, and the condition must be stated in the purchase order because heat treatment changes both the mechanical properties and the permitted fabrication sequence.
Ultrasonic examination to an agreed acceptance class for internally sound plate.
Charpy V-notch impact testing, including test temperatures below the standard requirement.
Z-direction testing in Z15, Z25 or Z35 quality for heavily restrained welded joints.
Simulated post-weld heat treatment followed by mechanical testing for reactor service.
Third party inspection and dimensional or surface acceptance to the purchaser's specification.
Applications in Boilers, Reactors and Storage Vessels
The grade is selected where pressure, temperature and process medium combine. Typical duties include:
Chemical reaction vessels, including ammonia synthesis towers operating around 30 MPa and 450 C, and polymerisation reactors.
Petrochemical towers and drums such as rectification and absorption columns, hydrotreating and high pressure hydrogenation reactors.
Storage tanks for crude oil and process liquids at ambient temperature, together with pressure vessel shells and heads.
Heat exchange equipment, where shell and tube exchanger shells and tube sheets must resist alternating thermal shock and avoid weld cracking from repeated temperature cycling.
Metallurgical plant: blast furnace hot blast stove shells, which contain hot blast at roughly 0.5 - 1.5 MPa and up to about 1200 C, and autoclaves used in hydrometallurgical leaching, where the vessel must also resist acid attack.
One point of clarification matters for specification writers. C-Mo plate of this type is a high temperature material, not a cryogenic one. Vessels storing liquefied natural gas at about -162 C require 9 % nickel steel or austenitic stainless steel, because a ferritic 0.3 % molybdenum plate does not have the notch toughness for that service.
Equivalent Grades and the Risk of Loose Cross Reference
| System | Designation | Relationship |
|---|---|---|
| EN 10028-2 | 16Mo3 | Direct modern successor for plate |
| DIN 17175 | 15Mo3 | Same grade family in seamless tube form |
| EN 10216-2 | 16Mo3 | Current seamless tube designation |
| UNI 5869 | 15Mo3 | Italian designation of the same grade |
| ASTM A204/A204M | Grade B | Similar application, different chemistry, not interchangeable |
Cross reference to the ASTM A204 grades should be treated with care. Those grades carry a molybdenum range of about 0.45 - 0.60 %, which is substantially higher than 15Mo3, so the two are not a one for one substitution even though both are used in elevated temperature pressure equipment. Where a project requires a formally equivalent material, the EN 10028-2 route is the defensible one. In design, the allowable stress of the plate at the metal design temperature must be taken from the code table used for the vessel, and the practical upper limit for this steel family is commonly taken as approximately 530 C.
Frequently Asked Questions
Q: What is 15Mo3 steel equivalent to?
EN 10028-2 16Mo3 is the direct modern equivalent for plate, and EN 10216-2 16Mo3 covers the seamless tube form. Older national designations such as UNI 5869 15Mo3 refer to the same grade family.
Q: Is 15Mo3 the same as 16Mo3?
The composition and mechanical properties are effectively the same 0.25 - 0.35 % molybdenum C-Mo steel. The difference is the standard: 15Mo3 comes from the withdrawn DIN 17155, while 16Mo3 is specified in the current EN 10028-2.
Q: Is 15Mo3 suitable for low temperature LNG storage?
No. Liquefied natural gas service at about -162 C requires 9 % nickel steel or austenitic stainless steel. 15Mo3 is intended for elevated temperature service in boilers, reactors and heat exchangers.
Q: What is the maximum service temperature of 15Mo3?
Design practice for this steel family normally limits it to approximately 530 C. The allowable stress at the design metal temperature must be read directly from the pressure vessel code table being applied.
Q: In what condition is 15Mo3 plate supplied?
Normalised is the standard condition for boiler and pressure vessel service. As rolled, thermo-mechanically controlled rolled and quenched and tempered plate can also be supplied when the specification allows.
Q: Which tests can be added to a 15Mo3 plate order?
Ultrasonic examination, Charpy V-notch impact testing at agreed temperatures, Z-direction testing in Z15, Z25 or Z35 quality, simulated post-weld heat treatment with mechanical testing, and third party inspection.