SA543GrBCl1/SA543GrBCl2/SA543GrBCl3 Steel Plate is a quenched and tempered Ni-Cr-Mo alloy steel plate designed for pressure vessels and other pressure equipment. It is primarily used for welded pressure vessels and components in the quenched and tempered (QT) condition. These alloy steels are typically specified for structures requiring steel plates with a thickness of 50mm or greater, falling under the category of American standard pressure vessel steels.
Key Features:
High tensile strength and toughness.
Suitable for high-pressure and high-temperature environments.
Commonly used in large industrial equipment, such as gas turbine components, nuclear reactors, and petrochemical processing plants.
Key Details:
Material Type: Quenched and tempered Ni-Cr-Mo alloy steel plate for pressure vessels and boilers.
Standards: Complies with ASTM A543/A543M (or ASME SA-543/SA-543M).
Delivery Condition: Typically supplied in quenched and tempered (QT) condition, but may also be available in normalized, normalized + tempered, or controlled rolling conditions upon request.
Chemical Composition:
Nickel (Ni): 0.40–0.70%
Chromium (Cr): 0.80–1.10%
Molybdenum (Mo): 0.45–0.60%
Carbon (C): ≤0.25%
Manganese (Mn): 1.15–1.50%
Silicon (Si): 0.15–0.50%
P & S: ≤0.025% (P), ≤0.010% (S)
Mechanical Properties:
Tensile Strength: 620–795 MPa (Class 2)
Yield Strength: ≥485 MPa
Elongation: ≥18%
Impact Toughness: Charpy V-notch tested at -20°C or lower (varies by class).
Process Performance:
Excellent weldability and formability.
Suitable for high-pressure and high-temperature applications (e.g., nuclear reactors, petrochemical plants).
Ordering Requirements: Specify thickness, dimensions, heat treatment, and additional tests (e.g., ultrasonic testing).
Applications:
Nuclear power: Reactor pressure vessels, steam generators.
Petrochemical: Reactors, heat exchangers, high-pressure piping.
Power plants: Boiler drums, turbine components.
Notes:
Class 1 (CL1): Lower tensile strength (105 ksi/725 MPa).
Class 2 (CL2): Intermediate strength (115 ksi/795 MPa).
Class 3 (CL3): Higher strength (90 ksi/620 MPa).
Delivery Condition and Heat Treatment of SA543GrBCl1/SA543GrBCl2/SA543GrBCl3 Steel Plates
Quenching and tempering. The plates shall be delivered in the quenched and tempered condition unless otherwise agreed between the steel mill and the purchaser or fabricator.
All plates shall undergo heat treatment. The plates shall be heated to the appropriate austenitizing temperature, held for sufficient time to ensure uniform temperature throughout the thickness, and then quenched using suitable liquid media by either spraying or immersion methods. Following quenching, the plates shall be tempered by heating to a temperature no lower than 595°C to achieve the required properties. The holding time during tempering shall be no less than 1.2 minutes per millimeter of thickness, but not less than 0.5 hours.
For plates with thickness exceeding 100mm, pre-normalizing or water quenching shall be performed within the temperature range of 900-1010°C prior to the specified heat treatment.
If the purchaser specifies the above heat treatment, the supplier shall temper the plates at a temperature no lower than 595°C prior to delivery.
material strictly in full compliance with ASME SEC. VIII DIV.2 requirements
The material shall conform to the following specifications:
Impact Testing at -29°C (Section 3.11.3.2 Impact Testing):
Preparation of Test Specimens: All test specimens shall be prepared from the material in its final heat-treated condition in accordance with 3.11.7.2.
Number of Impact Tests and Test Specimens:
One Charpy V-notch impact test shall consist of three specimens.
For as-rolled plates, one test from each plate.
For heat-treated plates (normalized, normalized and tempered, quenched and tempered), one test from each plate in the heat-treated condition.
For bars, pipe, tubing, rolled sections, forged parts or castings, one test from each heat treatment lot.
The number of impact tests shall not be less than the requirements of the material specification.
Locations and Orientation of Test Specimens:
Same as required by 3.11.7.2 and 3.11.7.3.
Specimens from plates shall be transverse to the final direction of rolling.
For forgings and pipe, transverse to the direction of major work (see Figure 3.14).
Minimum Lateral Expansion: As per 3.11.2.1(b)(2).
Retesting: Shall be in accordance with 3.11.7.6.