S275jr belongs to the European standard low alloy high strength steel plate, s275jr steel plate implementation standard for: en10025 special technical conditions.
S" is the abbreviation of structural steel;
"275" refers to the minimum yield strength (MPa) of steel thickness ≤ 16 mm;
"JR" denotes the quality grade related to the Charpy impact test energy value (27 J, room temperature 20°C);
1.0044 is the steel grade S275JR.
Chemical composition % of steel S275JR (1.0044):
| C | Mn | P | S | N | Cu | CEV |
| max 0.22 | max 1.5 | max 0.04 | max 0.04 | max 0.012 | max 0.55 | max 0.42 |
Mechanical properties of steel S275JR (1.0044):
| Nominal thickness (mm): | to 3 | 3 – 100 | 100 – 150 | 150 – 250 |
| Rm - Tensile strength (MPa) Flat and long products | 430-580 | 410-560 | 400-540 | 380-540 |
| Nominal thickness (mm): | to 16 | 16 – 40 | 40 – 63 | 63 – 80 | 80 – 100 | 100 – 150 | 150 – 200 | 200 – 250 |
| ReH - Minimum yield strength (MPa) Flat and long products | 275 | 265 | 255 | 245 | 235 | 225 | 215 | 205 |
| KV - Impact energy (J) longitud., | -20° 27 |
0° 27 |
+20° 27 |
| Nominal thickness (mm): | to 1 | 1 – 1.5 | 1.5 – 2 | 2 – 2.5 | 2.5 – 3 |
| A - Min. elongation Lo = 80 mm (%) parallel, | 15 | 16 | 17 | 18 | 19 |
| Nominal thickness (mm): | 3 – 40 | 40 – 63 | 63 – 100 | 100 – 150 | 150 – 250 |
| A - Min. elongation Lo = 5,65 √ So (%) parallel, | 23 | 22 | 21 | 19 | 18 |