High Strength Steel Plates: S690Q S690QL Q690D Q690E Q960E S960Q S960QL

Dec 04, 2025 Leave a message

S690QL-QUALITY-CERTIFICATE.pdf

High strength steel plates in the 690 MPa and 960 MPa yield classes are supplied under two parallel designation systems: the European S-series defined in EN 10025-6, and the Chinese Q-series defined in GB/T 16270 for quenched and tempered plate. Both systems use a letter suffix to indicate the impact test temperature, and that suffix usually decides which grade a project should order.

S690Q, S690QL and S690QL1 cover the 690 MPa class at impact test temperatures of -20 °C, -40 °C and -60 °C. Q690D and Q690E cover the same strength level under the Chinese standard with -20 °C and -40 °C toughness. At the top of the range, S960Q and S960QL provide a 960 MPa minimum yield strength, with Q960E as the Chinese equivalent of the low temperature variant.

The S690Q, Q690D and S960Q Family Explained

The designation carries three pieces of information. The leading letter shows the standard family: S for the European structural steel series and Q for the Chinese high strength series. The number is the minimum yield strength in megapascals. The trailing letter or letter pair shows the impact test temperature, and this is the part of the designation that is most often misunderstood.

In the EN 10025-6 system the suffix Q means a quenched and tempered delivery condition tested at -20 °C, QL adds a -40 °C impact requirement and QL1 adds -60 °C. In GB/T 16270 the quality letter works in steps of 20 °C, so Q690C is tested at 0 °C, Q690D at -20 °C, Q690E at -40 °C and Q690F at -60 °C. Choosing a colder suffix always means a more heavily alloyed and more tightly processed plate, which is why both price and welding controls rise with the number of letters.

690 MPa class: S690Q, S690QL, S690QL1 and Q690C, Q690D, Q690E, Q690F.

890 MPa class: S890Q, S890QL, S890QL1 and Q890C, Q890D, Q890E, Q890F.

960 MPa class: S960Q, S960QL and Q960C, Q960D, Q960E, Q960F.

Mechanical Properties Compared

The table below collects the minimum values normally quoted for these grades. They apply within the standard plate thickness range, and thickness has a mild effect on the yield strength guaranteed for quenched and tempered plate.

Property Q690D Q690E Q960E S690Q S690QL S690QL1 S960Q S960QL
Yield strength Rp0.2, min (MPa) 690 690 960 690 690 690 960 960
Tensile strength (MPa) 770-940 770-940 1050-1250 770-940 770-940 770-940 1050-1250 1050-1250
Elongation A5, min (%) 14 14 12 14 14 14 12 12
Impact test temperature (°C) -20 -40 -40 -20 -40 -60 -20 -40
Impact energy KV, min (J) 34 34 34 30 40 40 30 40
Hardness (HB) 220-280 220-280 280-350 220-280 220-280 220-280 280-350 280-350

Two patterns are worth noting. Impact energy rises from 30 J at -20 °C to 40 J at -40 °C and -60 °C in the European series, so the tougher grades are not simply colder versions of the same product. Hardness also climbs with the strength class, from 220-280 HB in the 690 MPa grades to 280-350 HB at 960 MPa, which is a practical indicator of how the plate will behave in machining, drilling and forming.

Chemical Composition and Carbon Equivalent

Composition limits explain most of the difference in fabrication behaviour between the grades, and the carbon equivalent is the single number that fabrication planners look at first.

Element (max, wt.%) Q690D and Q690E Q960E S690Q, S690QL and S690QL1 S960Q and S960QL
C 0.20 0.20 0.22 0.22
Si 0.60 0.60 0.86 0.86
Mn 1.80 1.80 1.80 1.80
P 0.025 0.025 0.030 0.030
S 0.020 0.020 0.020 0.020
Nb + V + Ti 0.12 0.22 0.12 0.22
Carbon equivalent Ceq 0.45 0.50 0.45 0.50

A 690 MPa plate held at or below a carbon equivalent of 0.45 keeps preheat requirements moderate, while the 960 MPa grades at up to 0.50 demand more careful thermal control during welding and, in thick sections, a defined preheat before the first pass. Chromium, nickel and molybdenum are added as required to guarantee hardenability in the thicknesses supplied, and the micro-alloying total is deliberately limited because an excess of niobium, vanadium or titanium would damage toughness.

Choosing a Grade by Temperature, Load and Welding

Grade selection follows a short sequence: confirm the design yield class, fix the impact test temperature from the minimum service temperature with a safety margin, and then check that the chosen grade is available in the required thickness with a delivery condition that suits the fabrication schedule.

Selection dimension Recommendation
Standard family Q-series for domestic projects; S-series for projects specified to European standards or destined for export
Service temperature Down to -20 °C: Q690D, S690Q, Q960D, S960Q. Down to -40 °C: Q690E, S690QL, Q960E, S960QL. Down to -60 °C: the QL1 grades
Load class 690 MPa class for mainstream heavy structures and mobile machinery; 960 MPa class for extreme load paths and maximum weight saving
Cost budget Economical starting point is Q690D or S690Q; premium options are S690QL1 and Q960E
Welding difficulty The 690 MPa class is easier to weld than the 960 MPa class; a preheat of at least 150 °C for 690 MPa grades and at least 200 °C for 960 MPa grades is a common starting point for thick plate

Where the service temperature is close to a grade boundary, moving one step colder is usually cheaper than adding a weldability risk to the project. Where the design margin is generous, staying with the warmer grade reduces preheat, consumable cost and heat input control on site.

Supply Range and Delivery Condition

Thickness capability differs between standards and strength classes, because a higher strength class needs higher hardenability to be guaranteed through a thick section. The table below shows representative supply limits and the delivery condition normally used.

Steel grade Standard Thickness (mm) Delivery condition
Q420B/C/D/E GB/T 1591 up to 150 TMCP or normalised
S460M/ML EN 10025-4 up to 100 TMCP
S460N/NL EN 10025-3 up to 200 Normalised
S460Q/QL/QL1 EN 10025-6 up to 150 Quenched and tempered
Q500C/D/E, Q550C/D/E GB/T 1591 up to 150 TMCP or quenched and tempered
Q690C/D/E GB/T 16270 up to 220 Quenched and tempered
S690Q/QL/QL1 EN 10025-6 up to 220 Quenched and tempered
Q890C/D/E GB/T 16270 up to 150 Quenched and tempered
S890Q/QL/QL1 EN 10025-6 up to 150 Quenched and tempered
Q960C/D/E GB/T 16270 up to 100 Quenched and tempered
S960Q/QL EN 10025-6 up to 100 Quenched and tempered
A514 Gr B/E/F/H/Q ASTM A514 up to 200 Quenched and tempered

Plate supplied in the quenched and tempered condition must not be reheated above its tempering temperature during fabrication, so any post-weld heat treatment has to be agreed before the order is placed. Thermal cutting and machining are both routine, but the higher hardness of the 960 MPa grades calls for preheating of the cut zone in thick plate and for carbide tooling with rigid setups.

Frequently Asked Questions

Q: What does the letter suffix mean in S690QL?
The Q indicates a quenched and tempered delivery condition with impact testing at -20 °C, adding L moves the impact test temperature to -40 °C, and QL1 moves it to -60 °C.

Q: Is Q690E the same as S690QL?
They are equivalent in strength and impact temperature but belong to different standards. The European grade limits phosphorus to 0.030 percent while the Chinese grade limits it to 0.025 percent, so certificates and welding procedures are not interchangeable without review.

Q: Which grade should be used at -40 °C service temperature?
Q690E, S690QL, Q960E and S960QL are all tested at -40 °C. The choice between them depends on whether the design needs the 690 MPa or the 960 MPa yield class.

Q: Can S690Q be welded without preheat?
Thin plate with a low carbon equivalent can sometimes be welded with minimal preheat, but a preheat of at least 150 °C is a common starting point for thick sections, and at least 200 °C for the 960 MPa grades.

Q: What is the maximum thickness available?
The Q690 and S690 grades are normally available up to 220 mm and the 960 MPa grades up to 100 mm, subject to mill capability and to the property requirements of the ordered thickness.

Q: Why is impact energy higher for S690QL than for S690Q?
Moving the test temperature down to -40 °C requires a cleaner, more heavily alloyed steel, and the specification reflects that with a minimum absorbed energy of 40 J instead of 30 J.

Q: Can these grades be used for pressure vessels?
They are structural steel grades intended for load-bearing structures. Pressure containment requires steel qualified to dedicated pressure vessel specifications, so the two families should not be substituted for one another.