DNV Grade D steel plate is common strength shipbuilding plate which is mainly used for built hull of vessels,ship body construction.Normally when rolling,Air rolled and Control Rolled is ok for ship plate DNV Grade D with the thickness equal and belows 40 Millimeters,and for thickness above 40mm,the heat treatment shall be Normalised or TMCP,these two technical treatment would improve steel strength in yield and tensile points for shipbuilding steel plate DNV Grade D.
Steel Standard:DNV (Det Norske Veritas)
Rolling Type:Shipbuilding steel plate,Common strength ship plate
Thickness:3mm-300mm
Width:1200mm-4200mm
Length:3000mm-18000mm
Heat Treatment:As Rolled/Control-rolled/TMCP/Normalised
Chemical Composition
|
DNV GRADE D general Strength Chemical Composition |
|||||||
|
Grade |
The Element Max (%) |
||||||
|
C |
Si |
Mn |
P |
S |
Al |
N |
|
|
DNV GRADE D |
0.21 |
0.10-0.35 |
0.60 |
0.035 |
0.035 |
0.015 |
|
|
Nb |
V |
Ti |
Cu |
Cr |
Ni |
Mo |
|
|
|
|
|
|
|
|
|
|
Mechanical Property
|
DNV GRADE D general strength property |
|||||||
|
Grade |
|
Mechanical Property |
Charpy V Impact Test |
||||
|
Thickness |
Yield |
Tensile |
Elongation |
Degree |
Energy 1 |
Energy 2 |
|
|
DNV GRADE D |
mm |
Min Mpa |
Mpa |
Min % |
-20 |
J |
J |
|
t≤50 |
235 |
400-520 |
22% |
20 |
27 |
||
|
50<t≤70 |
235 |
400-520 |
22% |
24 |
34 |
||
|
70<t≤150 |
235 |
400-520 |
22% |
27 |
41 |
||
|
Note: Energy 1 is transverse impact test, Energy 2 is longitudinal |
|||||||