S355J2W vs S355J2WP Steel Plate: Designation, Phosphorus and Toughness Explained

Nov 24, 2025 Leave a message

Decoding the two designations

Both S355J2W and S355J2WP are European standard atmospheric corrosion resistant structural steels supplied under EN 10025-5, and both are read the same way for most of their length. S means structural steel. 355 is the minimum yield strength in MPa. J2 means the steel is impact tested at minus 20 degrees Celsius with a minimum absorbed energy of 27 J. W means the steel has improved atmospheric corrosion resistance - it is a weathering steel. Only the final letter differs, and that letter is the whole story: P stands for phosphorus.

S355J2W is an improved atmospheric corrosion resistant structural steel with a low, residual phosphorus content. S355J2WP is the high-phosphorus variant, in which phosphorus is deliberately alloyed in the range 0.05-0.16 % to strengthen the protective oxide layer that forms on the surface in service. Both are weldable structural steels for exposed structures, and both are commonly supplied with a verified impact value at minus 20 degrees Celsius because of the J2 suffix.

The EN 10025-5 weathering steel family

These two grades sit inside a defined family of atmospheric corrosion resistant structural steels, which includes S235J0W, S235J2W, S355J0W, S355J2W, S355J0WP, S355J2WP and S355K2W. The pattern repeats across the family: the number is the minimum yield strength, the J symbol with its digit gives the impact test temperature, and the final W or WP shows whether the grade is a normal weathering steel or the high-phosphorus variant.

The W grades are further defined by their alloying philosophy. Some, such as S355J2W, are fine grain steels with a low phosphorus content, and they are used where toughness, weldability and forming must be combined with weather resistance. Others, such as S355J2WP, rely on phosphorus, copper and chromium to achieve their corrosion resistance. The choice between them is therefore a metallurgical choice, not simply a strength choice, because strength and impact class are identical.

Chemical composition: the phosphorus difference

Element, % S355J2W S355J2WP
C, max Low carbon, structural limit 0.15
Si, max Structural limit 0.80
Mn, max Structural limit 1.10
P Residual maximum only 0.05-0.16
S, max Low sulphur, fine grain practice 0.035
Cr Weathering addition 0.25-1.35
Cu Weathering addition 0.20-0.60

The table makes the distinction clear. In S355J2W, phosphorus is treated as an impurity and is held at a residual maximum; the corrosion resistance comes from copper, chromium and the other weathering additions combined with a fine grain structure. In S355J2WP, phosphorus is an intentional alloying element held between 0.05 % and 0.16 %, supported by chromium in the range 0.25-1.35 % and copper in the range 0.20-0.60 %. That high phosphorus level raises the atmospheric corrosion resistance further, but it also affects toughness and weldability, which is precisely why the standard pairs it with controlled carbon, silicon and manganese limits and why welding procedures for the WP grade need more attention.

Mechanical properties and impact toughness

Property S355J2W S355J2WP
Minimum yield strength 355 MPa 355 MPa
Impact test temperature minus 20 degrees Celsius minus 20 degrees Celsius
Minimum absorbed energy 27 J 27 J

Mechanically the two grades are interchangeable on paper: same minimum yield strength of 355 MPa in the normal thickness range, same impact test temperature of minus 20 degrees Celsius and the same minimum Charpy V-notch energy of 27 J on longitudinal specimens. The difference shows up in fabrication, not in the datasheet. The high phosphorus content of S355J2WP tends to increase strength slightly and reduce ductility and weldability in the heat-affected zone, while S355J2W, as a fine grain steel, offers the better balance of toughness and welding behaviour for heavily welded structures.

Applications of each grade

S355J2W: fine grain weathering steel used for high-speed railway bogies, welded frames, bolted and riveted structures, bridges and other welded assemblies where both weather resistance and dependable low-temperature toughness are required.

S355J2WP: high-phosphorus weathering steel used for exposed structures where atmospheric corrosion resistance is the leading requirement and welding is less severe, such as containers, transport equipment, towers, poles and architectural steelwork.

Both grades: exposed bridges, industrial and building structures, mast and gantry work, and any application where an unpainted steel surface is expected to develop a stable protective patina.

Neither grade should be used where the steel is permanently wet, immersed, buried or exposed to heavy chlorides or aggressive chemicals, because the protective oxide layer needs alternating wet and dry conditions to form and remain stable.

Ordering, delivery condition and designation

Weathering steel plates are normally ordered in the as-rolled condition, but the standard allows a specified delivery condition to be requested. When the steel is required to be supplied in a normalised or as-rolled condition, the symbols N or AR are added to the steel name and steel number; for example, a plate ordered with a specified minimum yield strength of 355 MPa, an impact energy of 27 J at 0 degrees Celsius, improved atmospheric corrosion resistance and a normalised delivery condition is designated S355J0W+N, or by its steel number with the same suffix. The same convention applies to the J2 grades discussed here, so the purchase order should always state the grade, the delivery condition, the plate thickness, the impact requirement and the required inspection certificate.

Practical ordering points:

Confirm the grade letter exactly - W and WP are not interchangeable, because the phosphorus level changes the corrosion performance and the welding behaviour.

State the impact class with the grade; the J2 symbol is the reason these plates can be used in low-temperature service.

Specify the delivery condition using the N or AR suffix where the fabrication route requires it.

Require the inspection certificate so that the impact test result, the chemistry and the corrosion-related alloying elements are documented for the project file.

Frequently asked questions

Q: What does the P in S355J2WP mean?
The P stands for phosphorus. S355J2WP is the high-phosphorus weathering variant, with phosphorus deliberately held in the range 0.05-0.16 % to strengthen the protective oxide layer, while S355J2W keeps phosphorus at a residual maximum.

Q: Are S355J2W and S355J2WP the same strength?
Yes. Both have a minimum yield strength of 355 MPa, an impact test temperature of minus 20 degrees Celsius and a minimum absorbed energy of 27 J, so the difference between them is chemistry and fabrication behaviour rather than load capacity.

Q: What does the designation S355J2W mean in full?
S means structural steel, 355 is the minimum yield strength in MPa, J2 requires impact testing at minus 20 degrees Celsius with a minimum of 27 J, and W indicates improved atmospheric corrosion resistance.

Q: Which grade is better for welded structures?
S355J2W is generally the better choice for heavily welded work. As a fine grain weathering steel with low residual phosphorus it offers a better balance of toughness and weldability, while the high phosphorus content of S355J2WP demands more control in the welding procedure.

Q: What does the suffix +N or +AR on the steel name mean?
It records the delivery condition. +N means the plate is supplied normalised and +AR means as-rolled. The symbol is added to the steel name and number so that the condition is unambiguous on the certificate.

Q: Can these steels be used unpainted?
Yes, in the right environment. In exposed atmospheric conditions with regular wet and dry cycles they form a stable protective rust layer and can be left unpainted. Permanent moisture, burial or heavy chloride exposure makes painting or coating necessary instead.

Q: Where is S355J2W typically used?
It is widely used for high-speed railway bogies, welded and bolted structural assemblies, bridges and other exposed structures that need both weather resistance and guaranteed toughness at low temperature.