Difference between RINA D420 and RINA D620 steel plate

Apr 10, 2026 Leave a message

RINA D420 is an extra-high-strength marine steel plate certified by the Italian classification society RINA (Registro Italiano Navale) for shipbuilding and offshore applications. The "D" grade signifies it is impact tested at -20°C . It has a minimum yield strength of 420 MPa and tensile strength ranging from 530 to 680 MPa, with a minimum elongation of 18% . The chemical composition is strictly controlled with carbon ≤0.20% and manganese ≤1.70% . This grade is typically supplied in normalized or quenched and tempered (QT) conditions and is available in thicknesses up to 260mm . It is widely used for hull structures, offshore platforms, and critical marine engineering components .

 

RINA D620 is an ultra-high-strength marine steel plate also certified by RINA, with impact toughness tested at -20°C . The "620" denotes a minimum yield strength of 620 MPa and tensile strength ranging from 720 to 890 MPa, with a minimum elongation of 15% . The chemical composition features carbon ≤0.20% and manganese ≤1.70%, with microalloying elements such as Nb, V, Ti, Cr, Ni, and Mo for enhanced properties . Impact energy requirements are minimum 41J (transverse) at -20°C . This grade requires advanced processing and is typically supplied in quenched and tempered (QT) or TMCP conditions . It is designed for the most demanding structural components in shipbuilding, ultra-deepwater offshore platforms, Arctic-class vessels, and FPSO units requiring maximum strength-to-weight ratio .

 

Both RINA D420 and RINA D620 are RINA-certified extra-high-strength marine steels with excellent low-temperature toughness tested at -20°C, ensuring reliable performance in harsh marine environments. Their primary difference lies in strength level: D420 offers a minimum yield strength of 420 MPa with tensile strength of 530-680 MPa, suitable for high-strength offshore platforms and general shipbuilding, while D620 provides a substantially higher minimum yield strength of 620 MPa with tensile strength reaching 720-890 MPa, designed for the most demanding load-bearing applications requiring maximum strength-to-weight ratio. Both grades feature controlled chemical composition with carbon ≤0.20% and maintain good weldability for critical marine service, though D620 requires more advanced processing like QT or TMCP to achieve its superior mechanical properties. 

 

RINA D420 extra high Strength Chemical Composition in Tempering and Quenching

 

Element

RINA D420 Max %

Element

RINA D420 Max %

C

0.20

Ni

0.40

Mn

1.70

Mo

0.08

Si

0.10-0.55

Al

0.020 min

S

0.030

Nb

0.20-0.05

P

0.030

V

0.05-0.10

Cu

0.35

Ti

0.0007-0.05

Cr

0.20

N

 

 

RINA D620 extra high Strength Chemical Composition in Tempering and Quenching

 

Element

RINA D620 Max %

Element

RID620 Max %

C

0.20

Ni

0.40

Mn

1.70

Mo

0.08

Si

0.10-0.55

Al

0.020 min

S

0.030

Nb

0.20-0.05

P

0.030

V

0.05-0.10

Cu

0.35

Ti

0.0007-0.05

Cr

0.20

N

 

 

RINA D420 extra high strength property in Tempering and Quenching

 

Grade

Thickness

Yield Strength

Tensile Strength

Elongation

Impact Energy

(mm)

MPa (min)

MPa

% (min)

(KV J) (min)

 

 

 

 

-20 degree

RINA D420

8-260

420

530-680

18

28J

 

RINA D620 extra high strength property in Tempering and Quenching

 

Grade

Thickness

Yield Strength

Tensile Strength

Elongation

Impact Energy

(mm)

MPa (min)

MPa

% (min)

(KV J) (min)

 

 

 

 

-20 degree

RINA D620

8-260

620

720-890

15

41J