A537 Class1 steel plate

Sep 08, 2025 Leave a message

ASTM-A537-A537M-Standard-Specification.pdf

General Product Description

The ASTM A537 specification is the Standard Specification for Pressure Vessel Plates, Heat-Treated, Carbon-Manganese-Silicon Steel used in the applications of fusion welded pressure vessels and structures. Typical applications are pressure vessels designed for moderate and lower-temperature service requiring excellent notch toughness as well as API 650 and API 620 storage tanks. 

 

Dimension Range

Hide/Show specific columns Edit

Thickness
(in)

Width
(in)

Length
(in)

0.375 - 2.00

72 - 123

240 - 600

Thickness: Inquire for thicknesses <0.375 in. and down to 0.197 in. and for thicknesses >2.00 in. up to 3.60.

Width: Inquire for widths <72 in. and down to 60 in. and for widths >123 in. up to 131.9 in.

Length: Inquire for lengths <240 in. down to 73 in and for lengths slightly >600 in.

 

Mechanical Properties

Tensile testing is performed in the transverse direction according to ASTM A20 requirements. The required mechanical properties are tabulated below:

Grade

Yield strength
(min ksi)

Tensile strength
(ksi)

Elongation in 2"
(min %)

Elongation in 8"
(min %)

A537 Class 1

50

70 - 90

22

18

Mechanical testing

Charpy V-Notch Impact Toughness requirements may be ordered as a supplementary requirement (S5). A minimum Charpy V-notch impact energy value of 30 ft-lbs [41 J] at - 40°F [-40°C] in longitudinal specimens is a typical supplemental impact toughness requirement. 

 

Chemical Composition

Meets chemical requirements of ASTM A537 Class 1/SA537 Class 1, as shown below. ASTM A20 limits apply to unspecified elements.

C
(max wt %)

Mn 1)
(max wt %)

P 2)
(max wt %)

S 2)
(max wt %)

Si
(max wt %)

Cu
(max wt %)

Ni 1)
(max wt %)

Cr
(max wt %)

Mo
(max wt %)

0.24

1.60

0.020

0.010

0.50

0.35

0.25

0.25

0.080

1) Manganese may exceed 1.35 % on heat analysis, up to a maximum of 1.60 %, and nickel may exceed 0.25 % on heat analysis, up to a maximum of 0.50 %, provided the heat analysis carbon equivalent (CEV) does not exceed 0.57 %.

2) P and S are more restrictive than A537/SA537 requirements. Even lower limits for P and S are available on an inquiry basis.

 

Carbon Equivalent

Thickness (in)

0.375 - 2.00

Typical CET (wt %)

0.31

Typical CEV (wt %)

0.43

Available Chemistries: Carbon equivalent (CEV) restrictions for weldability are available as a supplementary requirement (S20). Please inquire for additional chemistry restrictions.

Tolerances

Thickness, width, and length tolerances for A537 Class 1/SA537 Class 1 meet ASTM A20 requirements. The flatness tolerance for as-supplied product is ½ ASTM A20. Thicknesses <0.375" (0.250"-0.374") will only be supplied to full standard ASTM A20 flatness tolerance.

Delivery Conditions

ASTM A537 Class 1/ SA537 Class 1 is supplied in the normalized condition.