09CrCuSb Steel Plate for Sulphuric Acid Dew Point

Mar 06, 2024 Leave a message

09CrCuSb is a corrosion resistant low alloy steel plate developed for service in flue gas environments where sulphuric acid condenses on cold metal surfaces. The grade name records its characteristic chemistry: about 0.09 % carbon, together with chromium, copper and antimony as the elements that drive corrosion resistance. The nominal carbon content is deliberately low so that the plate remains weldable and formable despite its alloy additions.

The mechanism of protection is a protective oxide film that forms on the surface during service. Chromium and copper promote a dense, adherent layer that slows the diffusion of oxygen and corrosive species to the underlying metal, while antimony further stabilises the film in acid condensate. This is the reason the grade performs far better than ordinary carbon steel in the same environment.

Chemical Composition and Mechanical Properties

Chemistry is controlled by limits rather than a single target analysis, with low carbon, moderate chromium and copper content and a small but deliberate antimony addition. Sulfur and phosphorus are held low for weldability and toughness.

Property Typical requirement
Minimum yield strength Around 245 MPa and above
Tensile strength Approximately 390 MPa and above
Elongation after fracture 22 % or more
Corrosion behaviour Markedly lower metal loss than carbon steel in sulphuric acid dew point condensate

Grade designation follows the rules of GB/T 221, chemical analysis and tensile testing are carried out to GB/T 223 and GB/T 228.1 respectively, and impact testing where required follows GB/T 229. Dimensional tolerances for hot rolled plate are taken from GB/T 709, so thickness, width and flatness are controlled against a defined schedule rather than by local mill practice.

Delivery Condition and Surface Quality

The plate is supplied hot rolled, either as rolled or in a controlled rolling condition depending on the thickness and the mill route. Because the corrosion resistance depends on the chemistry rather than on a coating, surface condition and freedom from deep scale are the main visual acceptance criteria, and pickled or shot blasted supply can be arranged where a clean surface is needed for coating or inspection. Ultrasonic testing is available for plate used in pressure retaining parts of boilers and air preheaters.

Fabrication and Welding Notes

09CrCuSb is welded by the common arc processes with consumables whose composition and corrosion resistance are matched to the parent plate; a plain carbon steel weld metal would corrode preferentially in service and should be avoided. Preheat is generally modest for thin sections, and post weld heat treatment is applied where the design code requires it. Cold bending, rolling and flanging are straightforward. Thermal cutting leaves a normal cut edge that is dressed before welding. Because the protective film forms in service, the completed surface should not be contaminated by copper bearing tools or dissimilar metal deposits that could set up galvanic attack.

Applications

The grade is used for air preheater baskets and casing, economiser tubes and plates, boiler flue ducts, chimneys and stacks, gas-gas heaters, heat exchangers in waste incineration and desulfurisation plants, and heat recovery equipment where flue gas temperature falls below the acid dew point. It is also used for structural components exposed to acid rain and marine atmospheres.

Frequently Asked Questions

Q: Why does 09CrCuSb resist acid corrosion?

A: Chromium, copper and antimony promote a dense protective oxide film that forms in service and slows further attack by sulphuric acid condensate.

Q: Is it a weathering steel like Q355NH?

A: It is related in that it relies on a protective oxide layer, but it is designed for acid dew point condensate in flue gas rather than for general atmospheric exposure, and its chemistry and property targets differ.

Q: What weld consumables should be used?

A: Consumables that match the corrosion resistance of the parent plate. Using plain carbon steel weld metal creates a preferential corrosion path at the joint.

Q: Does the plate need a protective coating?

A: Not for the dew point corrosion mechanism itself, since the protective film forms in service, though coatings may be applied for appearance or for additional protection in severe locations.

Q: How is the plate tested and certified?

A: Chemical analysis, tensile testing and, when specified, impact testing are carried out to the relevant GB/T test method standards, with dimensional control to GB/T 709 and ultrasonic testing available on request.