Both Are Pressure Vessel Carbon Steels
Both A515 Gr.70 steel and A516 Gr.70 steel are carbon steel plates for pressure vessels, but they are intended for different temperature services and have different composition requirements.
Chemical Composition Comparison
A515 Gr.70 is a carbon-silicon steel: carbon up to 0.31 percent for thicknesses to 25 mm, increasing to 0.35 percent above 50 mm; manganese to 1.20 percent; silicon 0.15 to 0.40 percent; and phosphorus and sulfur to 0.035 percent. A516 Gr.70 has lower carbon of 0.27 to 0.30 percent depending on thickness, manganese of 0.85 to 1.20 percent, silicon of 0.13 to 0.45 percent, and phosphorus and sulfur to 0.035 percent.
Tensile Requirements
A515 Gr.70 has a minimum yield strength of 260 MPa and tensile strength of 485 to 620 MPa, with elongation of 17 percent in 200 mm and 21 percent in 50 mm. A516 Gr.70 has a tensile strength of 485 to 620 MPa, minimum yield strength of 260 MPa, and the same elongation requirements.
Application Differences
A515 Gr.70 carbon-silicon steel plates are primarily for intermediate- and higher-temperature service in welded boilers and other pressure vessels. A516 Gr.70 carbon steel plates are intended primarily for service in welded pressure vessels in moderate- and lower-temperature service, with fine-grain killed steel for better toughness.
Additional Differences
SA-516-70 has a maximum thickness of 204 mm, while SA515-GR-70 has a maximum thickness of 50 mm in the standard scope. A516 is supplied as fine-grain killed steel with improved low-temperature toughness, while A515 relies on higher carbon and silicon for elevated-temperature strength.
Frequently Asked Questions
Q: What is the difference between A515 and A516 Grade 70?
A: A515 is a carbon-silicon steel for intermediate and higher temperature service; A516 is a fine-grain killed carbon steel for moderate and lower temperature service.
Q: What are the tensile requirements of A515 Gr.70?
A: Yield strength of 260 MPa minimum and tensile strength of 485 to 620 MPa.
Q: What is the maximum thickness of A515 Gr.70?
A: 50 mm under the standard scope, versus 204 mm for A516-70.
Q: Which grade is used for high-temperature boilers?
A: A515 Gr.70, for intermediate and higher temperature service.
Q: Is A516 suitable for low-temperature service?
A: Yes, as fine-grain killed steel it provides good toughness for moderate and lower temperature service.
Q: Can they be used interchangeably?
A: No, the temperature service ranges and composition requirements differ.