What ASME SA387 Grade 22 Class 1 Steel Plate Is

ASME SA387 is a chromium-molybdenum alloy steel plate specification for welded boilers and pressure vessels operating at elevated temperature, technically identical to ASTM A387/A387M. The specification covers Grades 2, 5, 9, 11, 12, 21, 21L, 22, 22L and 91, and every grade is available in two strength levels, Class 1 and Class 2. The grades most often specified in refinery and power work are 11, 12, 22 and 5.

Grade 22 is the 2.25 % chromium, 1 % molybdenum steel, written in this article as chrome-moly plate. Class 1 denotes the lower-strength, higher-ductility condition of the grade, produced by normalising and tempering, and it is selected when forming severity, weldability or toughness requirements matter more than the highest available strength. Maximum thickness is governed only by the ability of the plate to meet the required mechanical properties.

Chemical Requirements for SA387 Grade 22

Both heat-analysis and product-analysis limits are controlled, which is important because chromium and molybdenum are the elements that determine elevated-temperature performance and hardenability.

Element Heat analysis, % Product analysis, %
Carbon, C 0.05 - 0.15 0.04 - 0.15
Manganese, Mn 0.30 - 0.60 0.25 - 0.66
Phosphorus, P 0.035 max 0.035 max
Sulphur, S 0.035 max 0.035 max
Silicon, Si 0.50 max 0.50 max
Chromium, Cr 2.00 - 2.50 1.88 - 2.62
Molybdenum, Mo 0.90 - 1.10 0.85 - 1.15

The nominal chromium content of Grade 22 is 2.25 % and the nominal molybdenum content is 1.00 %, values that place the steel in the standard 2.25Cr-1Mo family used for high-temperature hydrogen service equipment. The carbon range is deliberately narrow, between 0.05 % and 0.15 %, so that the plate can be welded and post-weld heat treated without developing excessive hardness.

Mechanical Properties: Class 1 and Class 2

Property Grade 22 Class 1
Tensile strength 515 - 690 MPa (75 to 100 ksi)
Yield strength, min, 0.2 % offset 310 MPa (45 ksi)
Elongation, min, 50 mm gauge length 18 %
Reduction of area, min 45 % on a round specimen, 40 % on a flat specimen
Property Grade 22 Class 1 Grade 22 Class 2
Tensile strength 515 - 690 MPa 585 - 760 MPa
Yield strength, min 310 MPa 415 MPa

Class 1 offers a minimum yield strength of 310 MPa and a tensile range of 515 MPa to 690 MPa with 18 % minimum elongation, while Class 2 raises the minimum yield strength to 415 MPa and the tensile range to 585 MPa to 760 MPa. The reduction-of-area minimum of 45 % on a round specimen and 40 % on a flat specimen confirms that Class 1 plate retains good through-thickness ductility, which is why it is often preferred for dished heads and for components that must tolerate thermal cycling.

Heat Treatment and Fabrication

Chrome-moly plate of this class is supplied normalised and tempered, and the tempering temperature is held above the intended post-weld heat treatment temperature so that properties are not degraded during fabrication. Welding is carried out with matching 2.25Cr-1Mo consumables, preheat, controlled interpass temperature and, for most production joints, a post-weld heat treatment that relieves stress and tempers the heat-affected zone. Forming is performed hot or cold depending on thickness, with heat treatment following any hot forming operation.

Normalising plus tempering as the standard delivery condition

Matching chromium-molybdenum welding consumables

Preheat and controlled interpass temperature during welding

Post-weld heat treatment for stress relief and zone stabilisation

Re-heat treatment after significant hot forming

Typical Service Applications

Hydroprocessing reactors, separators and high-temperature vessels

Heat exchangers and air coolers in refinery and petrochemical service

Steam drums, headers and high-temperature piping components

Equipment exposed to hydrogen at elevated temperature and pressure

Fabricated pressure parts where creep resistance is required beyond carbon steel limits

Because the grade is designed for elevated-temperature service, the allowable stress to be used in design should be taken from the appropriate code table for the exact grade and class rather than scaled from room-temperature tensile data.

Frequently Asked Questions

Q: What does Grade 22 mean in SA387?
Grade 22 is the 2.25 % chromium, 1 % molybdenum steel of the ASME SA387 specification, used for elevated-temperature pressure equipment.

Q: What is the difference between Class 1 and Class 2?
Class 1 has a minimum yield strength of 310 MPa and a tensile range of 515 MPa to 690 MPa; Class 2 is stronger, with a minimum yield strength of 415 MPa and a tensile range of 585 MPa to 760 MPa.

Q: Is SA387 Grade 22 the same as ASTM A387 Grade 22?
Yes. ASME SA387/SA387M is technically identical to ASTM A387/A387M, including the Grade 22 chemistry and both classes.

Q: Which heat treatment is used for Class 1 plate?
Plate is normalised and tempered, and the tempering temperature is selected to remain above the post-weld heat treatment temperature used during fabrication.

Q: Does the plate need post-weld heat treatment?
Chromium-molybdenum welds of this grade are normally post-weld heat treated to relieve residual stress and to temper the heat-affected zone, with the procedure qualified before production welding.

Q: Which grades of SA387 are most commonly ordered?
Grades 11, 12, 22 and 5 account for most demand, with Grade 22 widely used in refinery and petrochemical equipment for its combination of strength and high-temperature stability.