SA387 Grade 11 Class 2 steel plate

Sep 25, 2025 Leave a message

ASTM-A387-A387M.pdf

SA387 Grade 11 Class 2 is a ASME pressure vessel steel designed for high-temperature services, featuring a chrome-molybdenum alloy composition with chromium for oxidation and corrosion resistance. This specific class is noted for higher tensile and yield strengths compared to Class 1, making it suitable for demanding applications in the oil, gas, petrochemical, and chemical industries, as well as boilers and heat exchangers.

 

Equivalents

BS EN ASTM/ASME DIN
621 B ––– SA387-11-2 –––

 

Specifications for ASME SA387 Grade 11 Alloy Steel Plates

Chromium & Molybdenum content (according to the ASME specification)

Designation Nominal Chromium
Content (%)
Nominal Molybdenum
Content (%)
SA387 Grade 11 1.25% 0.50%

 

Tensile Requirements for ASME SA387 Grade 11 Alloy Steel Plates Class 2 Plates

Designation: Requirement: Grade 11
SA387 Grade 11 Tensile strength, ksi [MPa] 75 to 100 [515 to 690]
  Yield strength, min, ksi [MPa]/(0.2% offset) 43 [310]
  Elongation in 8 in. [200mm], min % 18
  Elongation in 2 in. [50mm], min, % 22
  Reduction of area, min % –––

 

Chemical Requirements for ASME SA387 Grade 11 Alloy Steel Plates

Element   Chemical Composition (%)
    SA387 Grade 11
Carbon: Heat Analysis: 0.05 - 0.17
  Product Analysis: 0.04 - 0.17
Manganese: Heat Analysis: 0.40 - 0.65
  Product Analysis: 0.35 - 0.73
Phosphorus: Heat Analysis: 0.035
  Product Analysis: 0.035
Sulphur (max): Heat Analysis: 0.035
  Product Analysis: 0.035
Silicon: Heat Analysis: 0.50 - 0.80
  Product Analysis: 0.44 - 0.86
Chromium: Heat Analysis: 1.00 - 1.50
  Product Analysis: 0.94 - 1.56
Molybdenum: Heat Analysis: 0.45 - 0.65
  Product Analysis: 0.45 - 0.70