SA 387 Gr 11 and SA 387 Gr 22 are both chromium-molybdenum (Cr-Mo) low-alloy steel plates certified to ASME SA-387/SA-387M, designed for high-temperature, high-pressure industrial applications (e.g., tube shell heat exchangers, petrochemical reactors, boilers). Their core difference lies in alloy content-directly impacting temperature resistance, mechanical strength, and corrosion performance. Understanding these distinctions is critical for selecting the right material for your project's severity, ensuring safety, and optimizing cost.
As a leading supplier of ASME-certified Cr-Mo steel plates and custom tube shell heat exchangers, GNEE breaks down the detailed differences between SA 387 Gr 11 and Gr 22 below.
Key Differences
Mechanical Properties: Strength & Toughness
The elevated alloy content in Gr 22 translates to superior mechanical performance, especially for high-pressure applications:
| Property (Class 2) | SA 387 Gr 11 | SA 387 Gr 22 |
|---|---|---|
| Yield Strength | 310 MPa | 345 MPa |
| Tensile Strength | 515–690 MPa | 550–700 MPa |
| Charpy V-Notch Toughness | ≥27 J (-29°C) | ≥27 J (-29°C) |
| Hardness (Max) | 207 HB | 237 HB |
Key Note: Both grades offer Class 1 (normalized + tempered) and Class 2 (quenched + tempered) options, but Class 2 is preferred for critical equipment due to higher strength. Gr 22 Class 2's Q&T parameters (higher quenching/tempering temps) further enhance its microstructure stability.
Corrosion Resistance: Sour Service & Hydrogen Attack
In petrochemical and oil & gas applications, resistance to corrosive media is critical:
SA 387 Gr 11: Meets NACE MR0175 standards for sour service (H₂S-containing environments) but is limited to moderate H₂S concentrations (≤10,000 ppm) and hydrogen partial pressures (≤10 MPa).
SA 387 Gr 22: Excels in harsh sour service and hydrogen-rich environments. Its higher Mo content forms a protective carbide layer that resists hydrogen-induced cracking (HIC) and SSCC, even at H₂S concentrations >10,000 ppm and hydrogen partial pressures >15 MPa.
Application Impact: Gr 22 is mandatory for hydrocracking reactors (high hydrogen pressure) and sour gas processing vessels, while Gr 11 suffices for moderate sour service (e.g., hydrotreating units).
Applications: Matching Grade to Operating Conditions
The performance differences directly align with distinct use cases-especially for core equipment like tube shell heat exchangers:
SA 387 Gr 11: Ideal for Moderate Harsh Environments
Tube shell heat exchangers in distillation, reboiling, and condensation units (500–593°C, 10–25 MPa).
Petrochemical hydrotreating reactors, medium-pressure separators, and boiler superheaters (≤593°C).
Sour service equipment with moderate H₂S/hydrogen levels (e.g., natural gas sweetening plants).
Cost-sensitive projects where Gr 22's extra performance is unnecessary.
GNEE's custom tube shell heat exchangers with Gr 11 plates are widely used in refineries and power plants for their balance of performance and cost.
SA 387 Gr 22: Ideal for Extreme Harsh Environments
Heavy-duty tube shell heat exchangers handling superheated steam, hot oil, or corrosive catalysts (600–649°C, 20–30 MPa).
Petrochemical hydrocracking reactors, catalytic cracking units, and ultra-high-pressure separators.
Power plant superheaters, reheaters, and heat recovery steam generators (HRSGs) in combined-cycle systems.
Offshore platform equipment (high hydrogen partial pressure + sour service).
Heat Treatment & Certification
SA 387 Gr 11:
Class 1: Normalized (899–927°C) + Tempered (620–650°C).
Class 2: Quenched (870–900°C) + Tempered (620–650°C).
Certifications: ASME SA-387, ASTM A387, NACE MR0175.
SA 387 Gr 22:
Class 1: Normalized (900–930°C) + Tempered (650–705°C).
Class 2: Quenched (900–930°C) + Tempered (650–705°C).
Certifications: ASME SA-387, ASTM A387, NACE MR0175, PED (European Pressure Equipment Directive) for EU projects.
Key Difference: Gr 22 requires higher heat treatment temperatures to fully optimize its alloy microstructure, ensuring consistent performance at extreme temps.
How to Choose Between SA 387 Gr 11 and Gr 22
Follow these guidelines to select the right grade:
Choose SA 387 Gr 11 If:
Your equipment operates at 500–593°C (1100°F) and pressure ≤25 MPa.
The process medium is moderately corrosive (low H₂S/hydrogen levels).
You need a cost-effective balance of performance and budget (e.g., general tube shell heat exchangers, medium-pressure vessels).
Choose SA 387 Gr 22 If:
Your equipment operates at 600–649°C (1200°F) or pressure ≥25 MPa.
The process medium is highly corrosive (high H₂S/hydrogen levels, sour service).
The equipment is safety-critical (e.g., hydrocracking reactors, ultra-high-pressure tube shell heat exchangers) where failure risks downtime or safety hazards.
GNEE's SA 387 Gr 11/Gr 22 Solutions
At GNEE, we supply ASME-certified SA 387 Gr 11 and Gr 22 plates tailored to industrial needs, with a focus on tube shell heat exchanger applications:
Key Offerings:
Certified Plates: Full compliance with ASME SA-387, ASTM A387, NACE MR0175, and PED. Traceable mill test reports (MTRs) included.
Custom Sizes: Thicknesses 6mm–250mm (Gr 11) and 6mm–300mm (Gr 22); widths up to 4600mm, lengths up to 12000mm.
Rigorous Testing: 100% ultrasonic testing (UT) per ASTM A578 Level B; optional HIC/SSCC testing for sour service.
Fabrication Integration: Custom tube shell heat exchangers using Gr 11/Gr 22 plates-engineered to your temperature/pressure requirements.
Global Support: Fast delivery (3–7 days for in-stock, 2–4 weeks for custom) and free technical consultation to confirm grade selection.
Conclusion
SA 387 Gr 11 and Gr 22 are both high-performance Cr-Mo steel plates, but their alloy content drives distinct capabilities:
- SA 387 Gr 11: The cost-effective choice for moderate high-temperature/pressure applications (≤593°C) like general tube shell heat exchangers and hydrotreating units.
- SA 387 Gr 22: The premium choice for extreme conditions (≥600°C, harsh sour service) like heavy-duty tube shell heat exchangers and hydrocracking reactors.
Choosing the wrong grade can lead to premature failure, costly downtime, or unnecessary expenses. For personalized guidance-whether you need to confirm grade suitability, request a quote, or design a custom tube shell heat exchanger-contact GNEE's engineering team today.
Get in touch with GNEE now to secure high-quality SA 387 Gr 11/Gr 22 plates and optimize your critical industrial equipment's performance!
What is ASTM A387 Grade 11 equivalent to?
ASME SA387 grade 11
ASTM A387 grade 11 equivalent steel is ASME SA387 grade 11. ASTM A387 grade 11 covers A387 grade 11 class 1 and A387 grade 11 class 2, which are equivalent to ASME SA387 grade 11 class 1 and SA387 grade 11 class 2 respectively.
What is SA 387 GR 12 Cl 2 equivalent material?
The Equivalent materials of Sa 387 Gr 12 are BS 620B, UNS K11757, A387 / SA 387, DIN 13 CRMO 44, and EN 3 CRMO 45.
What is the P number of SA 387 GR 11 material?
The ASME SA-387/ ASTM A387 Gr. 11 steel has the nominal composition of 1.25Cr-0.5Mo-Si with UNS designation number of K11789 and P number of 4.
Products Display



Packing&Shipping


Exhibitions and Customer Visits

GNEE Steel also supplies a variety of boilers and pressure vessel steel plates, such as A204 Grade B,A515 Grade 70,A537 Class 1,SA387 Grade 11 Class 1,P265GH,S537 Class 2,P355Q,P275N,P355N,P690Q,Q345R, etc. If you want to know more about other types of steel plates, you can call the consultation hotline at +8615824687445 or send an email to alloy@gneesteelgroup.com. You are welcome to consult us, and we are very willing to answer your questions.
| Grades Of Pressure Vessel Plates Supplied By GNEE | |||||
| ASTM | ASTM A202/A202M | ASTM A202 Grade A | ASTM A202 Grade B | ||
| ASTM A203/A203M | ASTM A203 Grade A | ASTM A203 Grade B | ASTM A203 Grade D | ASTM A203 Grade E | |
| ASTM A203 Grade F | |||||
| ASTM A204/A204M | ASTM A204 Grade A | ASTM A204 Grade B | ASTM A204 Grade C | ||
| ASTM A285/A285M | ASTM A285 Grade A | ASTM A285 Grade B | ASTM A285 Grade C | ||
| ASTM A299/A299M | ASTM A299 Grade A | ASTM A299 Grade B | |||
| ASTM A302/A302M | ASTM A302 Grade A | ASTM A302 Grade B | ASTM A302 Grade C | ASTM A302 Grade D | |
| ASTM A387/A387M | ASTM A387 Grade 5 Class1 | ASTM A387 Grade 5 Class2 | ASTM A387 Grade 11 Class1 | ASTM A387 Grade 11 Class2 | |
| ASTM A387 Grade 12 Class1 | ASTM A387 Grade 12 Class2 | ASTM A387 Grade 22 Class1 | ASTM A387 Grade 22 Class2 | ||
| ASTM A515/A515M | ASTM A515 Grade 60 | ASTM A515 Grade 65 | ASTM A515 Grade 70 | ||
| ASTM A516/A516M | ASTM A516 Grade 55 | ASTM A516 Grade 60 | ASTM A516 Grade 65 | ASTM A516 Grade 70 | |
| ASTM A517/A517M | ASTM A517 Grade A | ASTM A517 Grade B | ASTM A517 Grade E | ASTM A517 Grade F | |
| ASTM A517 Grade P | ASTM A517 Grade J | ||||
| ASTM A533/A533M | ASTM A533 Grade A Class1 | ASTM A533 Grade B Class1 | ASTM A533 Grade C Class1 | ASTM A533 Grade D Class1 | |
| ASTM A533 Grade A Class2 | ASTM A533 Grade B Class2 | ASTM A533 Grade C Class2 | ASTM A533 Grade D Class2 | ||
| ASTM A533 Grade A Class3 | ASTM A533 Grade B Class3 | ASTM A533 Grade C Class3 | ASTM A533 Grade D Class3 | ||
| ASTM A537/A537M | ASTM A537 Class1 | ASTM A537 Class2 | ASTM A537 Class3 | ||
| ASTM A612/A612M | ASTM A612 | ||||
| ASTM A662/A662M | ASTM A662 Grade A | ASTM A662 Grade B | ASTM A662 Grade C | ||
| EN | EN10028-2 | EN10028-2 P235GH | EN10028-2 P265GH | EN10028-2 P295GH | EN10028-2 P355GH |
| EN10028-2 16MO3 | |||||
| EN10028-3 | EN10028-3 P275N | EN10028-3 P275NH | EN10028-3 P275NL1 | EN10028-3 P275NL2 | |
| EN10028-3 P355N | EN10028-3 P355NH | EN10028-3 P355NL1 | EN10028-3 P355NL2 | ||
| EN10028-3 P460N | EN10028-3 P460NH | EN10028-3 P460NL1 | EN10028-3 P460NL2 | ||
| EN10028-5 | EN10028-5 P355M | EN10028-5 P355ML1 | EN10028-5 P355ML2 | EN10028-5 P420M | |
| EN10028-5 P420ML1 | EN10028-5 P420ML2 | EN10028-5 P460M | EN10028-5 P460ML1 | ||
| EN10028-5 P460ML2 | |||||
| EN10028-6 | EN10028-6 P355Q | EN10028-6 P460Q | EN10028-6 P500Q | EN10028-6 P690Q | |
| EN10028-6 P355QH | EN10028-6 P460QH | EN10028-6 P500QH | EN10028-6 P690QH | ||
| EN10028-6 P355QL1 | EN10028-6 P460QL1 | EN10028-6 P500QL1 | EN10028-6 P690QL1 | ||
| EN10028-6 P355QL2 | EN10028-6 P460QL2 | EN10028-6 P500QL2 | EN10028-6 P690QL2 | ||
| JIS | JIS G3115 | JIS G3115 SPV235 | JIS G3115 SPV315 | JIS G3115 SPV355 | JIS G3115 SPV410 |
| JIS G3115 SPV450 | JIS G3115 SPV490 | ||||
| JIS G3103 | JIS G3103 SB410 | JIS G3103 SB450 | JIS G3103 SB480 | JIS G3103 SB450M | |
| JIS G3103 SB480M | |||||
| GB | GB713 | GB713 Q245R | GB713 Q345R | GB713 Q370R | GB713 12Cr1MoVR |
| GB713 12Cr2Mo1R | GB713 13MnNiMoR | GB713 14Cr1MoR | GB713 15CrMoR | ||
| GB713 18MnMoNbR | |||||
| GB3531 | GB3531 09MnNiDR | GB3531 15MnNiDR | GB3531 16MnDR | ||
| DIN | DIN 17155 | DIN 17155 HI | DIN 17155 HII | DIN 17155 10CrMo910 | DIN 17155 13CrMo44 |
| DIN 17155 15Mo3 | DIN 17155 17Mn4 | DIN 17155 19Mn6 | |||