N06054 is a nickel based alloy plate grade identified by its Unified Numbering System designation. Its chemistry is built on nickel with substantial chromium and molybdenum additions and a very low carbon content. That combination is what distinguishes the alloy: chromium provides resistance to oxidising media and to high temperature oxidation, molybdenum provides resistance to reducing media and to chloride bearing environments, and the low carbon level keeps the corrosion resistant phase stable in the heat affected zone of a weld.
The alloy contains no deliberate tungsten addition, and its performance comes from the nickel chromium molybdenum balance rather than from a large number of alloying elements. That makes it a versatile material for plants where a single process stream may alternate between oxidising and reducing conditions.
Chemical Composition and Mechanical Properties
The nominal composition is nickel with roughly 22 to 24 % chromium, 15 to 16.5 % molybdenum and a controlled iron level, with carbon held at or below about 0.01 % and small additions of aluminium. The low carbon and low silicon content is deliberate, because it minimises the precipitation of secondary phases that would reduce corrosion resistance in the weld zone.
| Property | Typical requirement |
|---|---|
| Minimum yield strength | About 340 MPa |
| Minimum tensile strength | About 690 MPa |
| Elongation | 40 % or more |
| Grain size | Controlled fine grain for toughness and forming |
Plate, sheet and strip of low carbon nickel chromium molybdenum alloys are supplied against the relevant ASTM specification for this product family, with the UNS number being the defining grade identifier. Mechanical property requirements depend on product form and thickness, so the order should state the product form, the thickness and the applicable specification.
Corrosion Performance and High Temperature Behaviour
The alloy resists pitting, crevice attack and stress corrosion cracking in chloride bearing environments and performs well in mixed acid and in contaminated process streams containing chloride, which is why it is widely used in flue gas desulfurisation and in pulp and paper bleaching circuits. At elevated temperature it forms a protective oxide and retains strength, so it can be used for components exposed to hot process gas as well as to the aggressive condensate that forms when the gas cools. Like other nickel alloys it should not be used in contact with mercury, and service in strongly reducing or strongly oxidising extremes should be checked against corrosion data before the design is fixed.
Fabrication, Forming and Welding
N06054 is ductile and can be cold formed, machined and welded by the usual processes, though it work hardens quickly, so machining should use rigid tooling, low cutting speeds and generous lubrication. Welding should use matching filler metal and a high purity shielding gas, with clean, dedicated tooling to avoid iron contamination that would reduce corrosion resistance. Heat input should be controlled and preheat is not required; interpass temperature should be limited. After welding, oxide colour on the surface is usually removed by pickling or grinding, since contaminated scale is a starting point for corrosion. Post weld heat treatment is generally not needed for this low carbon grade, which is one of its practical advantages over higher carbon nickel alloys.
Applications
Typical uses include chemical process reactors, columns and heat exchangers, flue gas desulfurisation absorbers and ducting, pollution control equipment, pulp and paper processing vessels, waste incineration components, sour gas handling equipment and components exposed to mixed acid or chloride bearing streams.
Frequently Asked Questions
Q: What is the UNS N06054 alloy based on?
A: It is a nickel chromium molybdenum alloy with a very low carbon content, designed for resistance to both oxidising and reducing corrosive media.
Q: Does N06054 contain tungsten?
A: No. Its corrosion resistance comes from the nickel chromium molybdenum balance and its low carbon and low silicon content, not from a deliberate tungsten addition.
Q: Why is the carbon content kept so low?
A: A very low carbon level limits the formation of secondary phases in the weld heat affected zone, so welded joints retain corrosion resistance without requiring post weld heat treatment.
Q: Is the alloy difficult to machine?
A: It work hardens readily and needs rigid setups, sharp tooling, moderate to low cutting speeds and good lubrication, but with those conditions it machines predictably.
Q: How should the surface be treated after welding?
A: Oxide colour and any contamination should be removed by pickling, brushing or grinding with clean stainless tools, because a contaminated heat tint becomes a corrosion initiation site.