What LR DH69 Is
LR DH69 is an extra high strength hull structural steel approved under the Lloyd's Register Rules for the Manufacture, Testing and Certification of Materials. In the designation, D sets the Charpy impact test temperature at -20 °C, H identifies the higher strength category and the number fixes the strength level at a 690 MPa minimum yield strength. The grade is used for shipbuilding projects and for ocean offshore structural work, where the combination of very high strength and guaranteed toughness allows primary structure to be built lighter while still resisting brittle fracture. Compared with the E quality of the same strength level, the DH69 impact requirement is set 20 °C warmer, so it is selected for structures whose design temperature does not reach the colder window.
Chemical Composition
| Element | LR DH69 limit |
|---|---|
| Carbon | 0.20 % maximum |
| Silicon | 0.55 % maximum |
| Manganese | 1.70 % maximum |
| Phosphorus | 0.030 % maximum |
| Sulphur | 0.030 % maximum |
| Aluminium, total | 0.015 % minimum |
| Nitrogen | 0.020 % maximum |
| Niobium, vanadium, titanium | Microalloy additions within the range fixed by the society rules |
Aluminium is specified as a minimum because it deoxidises the steel and refines the grain, which is what makes the -20 °C impact requirement achievable at this strength level. The microalloying elements are added in small controlled amounts so that the strength is developed by controlled rolling and by the resulting fine grain structure rather than by extra carbon, which would damage weldability. Two parameters are calculated from the heat analysis and reported with the certificate: the crack sensitivity index Pcm = C + Si/30 + Mn/20 + Cu/20 + Ni/60 + Cr/20 + Mo/15 + V/10 + 5B and the carbon equivalent value CEV = C + Mn/6 + Cr/5 + Mo/5 + V/5 + Ni/15 + Cu/15.
Mechanical Properties and Charpy Requirements
| Thickness | Minimum yield strength | Tensile range | Minimum elongation | Impact at -20 °C |
|---|---|---|---|---|
| Up to 50 mm | 690 MPa | 770-940 MPa | 16 % | 46 J transverse, 69 J longitudinal |
| Over 50 to 70 mm | 690 MPa | 770-940 MPa | 16 % | 46 J transverse, 69 J longitudinal |
| Over 70 to 100 mm | 690 MPa | 770-940 MPa | 16 % | 46 J transverse, 69 J longitudinal |
The yield and tensile requirements are held constant to 100 mm, and impact testing is carried out at -20 °C in both the transverse and the longitudinal direction, with the higher energy requirement applied to longitudinal specimens. The gap between the 690 MPa yield strength and the 770-940 MPa tensile range gives a yield-to-tensile ratio below about 0.90, which is what keeps the material from losing plastic reserve as the strength rises.
Welding and Thick-Section Fabrication
A 690 MPa hull steel is welded under a qualified procedure from the first joint. Because the carbon and manganese ceilings are low and the design depends on microalloying rather than on carbon for strength, the carbon equivalent and the crack sensitivity index both stay low enough to keep preheat temperatures manageable, but thick sections still require preheat matched to the joint thickness, hydrogen-controlled consumables, a controlled interpass temperature and limits on heat input so that the coarse-grained heat-affected zone retains its toughness. Consumables are matched to the 770-940 MPa tensile band, and qualification of the procedure normally includes Charpy testing of weld metal and heat-affected zone at -20 °C. Cutting, forming and stress-relief operations are kept below any temperature that would degrade the delivered condition of the plate.
Testing, Certification and Supply
DH69 is a classed material, so every plate is issued with a certificate against the Lloyd's Register rules together with a mill test certificate carrying heat number, chemical analysis, microalloy content, tensile and yield results, elongation and Charpy energy at -20 °C in both orientations. Ultrasonic examination to an agreed acceptance class is standard for primary structure, thickness-direction testing to Z15, Z25 or Z35 can be added where welded joints transfer load through the plate thickness, and independent third-party inspection at the works is available when the owner or the yard requires it. Plate can be supplied in the quenched and tempered, thermomechanical controlled process, normalized or as-rolled condition, cut or beveled to the yard's block drawings, and shot blasted and primed to suit the painting system, then shipped by container or break bulk with grade, heat number and class stamp marked on each plate.
Frequently Asked Questions
Q: What does DH69 mean in the shipbuilding designation?
A: D indicates an impact test temperature of -20 °C, H indicates the higher strength category and 69 denotes the strength level, giving a 690 MPa minimum yield strength.
Q: How does LR DH69 differ from LR EH69?
A: The strength level is identical at a 690 MPa minimum yield and a 770-940 MPa tensile range. The difference is the impact test temperature, which is -20 °C for DH69 and -40 °C for EH69.
Q: What Charpy values apply to LR DH69?
A: A minimum of 46 J in transverse testing and 69 J in longitudinal testing at -20 °C, at the sampling frequency set by the society rules.
Q: Why are Pcm and carbon equivalent both reported?
A: The carbon equivalent value predicts hardenability in the heat-affected zone while Pcm predicts crack sensitivity in the weld. Both are calculated from the heat analysis and used to set preheat and consumable requirements.
Q: Which delivery conditions are available?
A: Quenched and tempered, thermomechanical controlled processed, normalized and as-rolled deliveries are produced, and the condition is agreed with the yard because it sets the limits for forming and welding heat input.
Q: What documentation is issued with the plate?
A: A Lloyd's Register certificate together with a mill test certificate showing heat number, chemical analysis, tensile and yield results, elongation and impact energy at -20 °C in both directions.