S355G7+N is a high-strength, low-alloy structural steel grade specified by the EN 10225 standard, designed primarily for offshore and marine applications.
Steel Standard:EN 10225
Rolling Type:Oil and offshore platform steel plate
Thickness:6mm-300mm
Width:1500mm-4200mm
Length:3000mm-18000mm
Heat Treatment:Normalized
S355G7+N Steel plate Chemical Composition
S355G7+N Chemical Composition | |||||||
Grade | The Element Max (%) | ||||||
C | Si | Mn | P | S | Al | N | |
S355G7+N | 0.14 | 0.15-0.55 | 1.0-0.01 | 0.02 | 0.01 | 0.0055 | 0.01 |
Nb | V | Ti | Cu | Cr | Ni | Mo | |
0.04 | 0.06 | 0.025 | 0.3 | 0.25 | 0.5 | 0.08 | |
Crack Sensitivity: Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent: Ceq = 【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%
S355G7+N Steel plate strength property
S355G7+N high strength property | |||||||
Grade |
| Mechanical Property | Charpy V Impact Test | ||||
Thickness | Yield | Tensile | Elongation | Degree | Energy 1 | Energy 2 | |
S355G7+N | mm | Min Mpa | Mpa | Min % | -40 | J | J |
t≤50 | 355 | 470-630 | 22% | 50 | 50 | ||
50<t≤63 | 355 | 470-630 | 22% | 50 | 50 | ||
63<t≤100 | 325 | 490-630 | 22% | 50 | 50 | ||
Note: Energy 1 is transverse impact test, Energy 2 is longitudinal | |||||||