P265GH and P295GH are two non-alloy pressure vessel steels defined by EN 10028-2. Both are widely used for boilers, pressure vessels, heat exchangers and piping, and both are specified for elevated temperature service. Choosing between them influences wall thickness, forming behaviour, welding procedure and, ultimately, the total cost of the equipment.
This comparison sets out the differences that matter in practice: chemical composition, mechanical properties, impact requirements, formability, welding parameters and typical applications.
Grade Designation and Standard Classification
Both grades are flat products covered by EN 10028-2, the part of the EN 10028 series that deals with non-alloy and alloy steels for pressure purposes with specified elevated temperature properties. The designation of each grade carries the same logic:
P – pressure application
265 / 295 – minimum yield strength ReH at room temperature, in MPa
G – grade
H – suitable for high temperature service
Both steels are fine grain killed steels, normally produced by electric furnace melting followed by secondary refining and vacuum degassing. They are supplied in the normalized or thermomechanical rolled condition so that a uniform fine grain structure and stable mechanical properties are obtained.
Chemical Composition Comparison
| Element (wt %) | P265GH | P295GH | Remark |
|---|---|---|---|
| C | 0.20 max | 0.08 – 0.20 | P295GH uses a controlled carbon range |
| Si | 0.40 max | 0.40 max | Identical |
| Mn | 0.70 – 1.40 | 0.90 – 1.50 | P295GH needs more manganese for strength |
| P | 0.025 max | 0.025 max | Identical |
| S | 0.010 max | 0.010 max | Identical |
| Al total | 0.020 min | 0.020 min | Grain refinement |
| Cr | 0.30 max | 0.30 max | Identical |
The higher manganese content of P295GH is the main compositional reason for its higher strength level, while the restricted carbon range keeps toughness under control. Sulphur and phosphorus are held to the same low limits in both grades because they reduce toughness and weldability.
Mechanical Properties Comparison
| Property | P265GH | P295GH | Remark |
|---|---|---|---|
| Yield strength ReH, min | 265 MPa | 295 MPa | Room temperature minimum |
| Tensile strength Rm | 410 – 560 MPa | 450 – 600 MPa | P295GH is the stronger grade |
| Elongation A, min | 24 % | 22 % | P265GH is more ductile |
| Charpy impact energy, min | 40 J at -20 °C | 40 J at 0 °C | P265GH has the better low temperature toughness |
The 30 MPa difference in minimum yield strength looks small, but it translates into a measurable reduction in required wall thickness at higher design pressure, which in turn lowers the weight of the finished vessel. Where low temperature toughness governs the design, the -20 °C impact requirement of P265GH is the decisive advantage.
Applications and Selection Guidelines
The two grades overlap in many services, so selection usually comes down to the governing design condition:
P265GH – low and medium pressure vessels, heat exchangers, storage tanks, boiler components and parts that must be cold formed into complex shapes
P295GH – higher pressure vessels, process equipment, power generation components and structures where higher strength allows a useful weight reduction
Practical guidance: choose P265GH when formability or low temperature toughness is the limiting factor, and choose P295GH when the design pressure is high enough that the extra 30 MPa of yield strength reduces plate thickness. Where both grades satisfy the design, the lower cost option is usually the one that best matches the available fabrication equipment.
Fabrication, Forming and Welding Considerations
Hot forming – both grades are hot formed in the range 850 to 1100 °C, followed by the appropriate heat treatment
Cold forming – P265GH performs better because of its lower yield strength and higher elongation
Welding – both steels weld readily with all common arc processes; preheating is applied for thicker sections, typically 100 to 150 °C above 20 mm for P265GH and 150 to 200 °C above 20 mm for P295GH
Post-weld heat treatment – recommended for both grades, normally carried out in the range 580 to 620 °C
Inspection – mill test certificates to EN 10204 3.1 or 3.2 confirm chemical composition, tensile properties and impact results for each heat
For both grades the welding procedure should be qualified for the actual thickness and heat input to be used, since the elevated temperature properties that make these steels suitable for pressure service also depend on the final microstructure after welding and heat treatment.
Frequently Asked Questions
Q: What is the main difference between P265GH and P295GH?
P265GH has a minimum yield strength of 265 MPa and P295GH has 295 MPa. P295GH also contains more manganese and is supplied with a controlled carbon range.
Q: Which standard covers both grades?
Both are defined by EN 10028-2, which specifies flat products of non-alloy and alloy steels for pressure purposes with elevated temperature properties.
Q: Which grade has better low temperature toughness?
P265GH is impact tested at -20 °C with a minimum of 40 J, while P295GH is tested at 0 °C, so P265GH is the better choice for colder service.
Q: Which grade is easier to form?
P265GH is easier to cold form because of its lower yield strength and higher minimum elongation of 24 %.
Q: What preheating is required for welding?
For sections above 20 mm, preheating is typically 100 to 150 °C for P265GH and 150 to 200 °C for P295GH, with post-weld heat treatment at 580 to 620 °C recommended for both.
Q: When should P295GH be selected?
Select P295GH for higher pressure vessels, process equipment and power generation components where the additional strength reduces wall thickness and total equipment weight.