DNV F620 shipbuilding steel plate and sheet which is the similar with LR Grade F620,GL Grade F620,NK F63,BV Grade F620,CCS Grade F620,RINA Grade F620,KR FQ63 which are the same and owned higher steel strength at minimum yield strength 620 Mpa and with tensile strength within 720-890 Mpa.Done low temperature impacting test for DNV F620 under minus 60 centigree when rolling.
Steel Standard:DNV (Det Norske Veritas)
Rolling Type:Extra high strength ship plate
Thickness:6mm-250mm
Width:1500mm-4200mm
Length:3000mm-18000mm
Heat Treatment:Quenched and Tempered
|
DNV F620 extra high Strength Chemical Composition |
|||||||
|
Grade |
The Element Max (%) |
||||||
|
C |
Si |
Mn |
P |
S |
Al |
N |
|
|
DNV F620 |
0.18 |
0.10-0.55 |
1.6 |
0.025 |
0.025 |
0.015-0.08 |
0.020 |
|
Nb |
V |
Ti |
Cu |
B |
Ni |
Mo |
|
|
0.02-0.05 |
0.04-0.10 |
0.02 |
|
0.005 |
|
|
|
|
DNV F620 extra high general strength property |
|||||||
|
Grade |
|
Mechanical Property |
Charpy V Impact Test |
||||
|
Thickness |
Yield |
Tensile |
Elongation |
Degree |
Energy 1 |
Energy 2 |
|
|
DNV F620 |
mm |
Min Mpa |
Mpa |
Min % |
-60 |
J |
J |
|
t≤50 |
620 |
720-890 |
15% |
41 |
62 |
||
|
50<t≤70 |
620 |
720-890 |
15% |
41 |
62 |
||
|
70<t≤150 |
620 |
720-890 |
15% |
41 |
62 |
||
|
Note: Energy 1 is transverse impact test, Energy 2 is longitudinal |
|||||||
Other Name
DNV Grade F620 Shipbuilding steel plate,DNV Grade F620 Ship Steel plate ,DNV Grade F620 Marine Steel plate , DNV Grade F620 Steel Plate .
Additional Condition
UT(Ultrasonic examination), AR(As Hot Rolled only), TMCP(Thermal Mechanical Control Processing), N(Normalized), Q+T(Quenched and Tempered),Z Direction Test(Z15,Z25,Z35), Charpy V-Notch Impact Test, The Third Party Test (such as SGS Test), Coated or Shot Blasting and Painting.