Steel Standard:DNV (Det Norske Veritas)
Rolling Type:Extra high strength ship plate
Thickness:6mm-250mm
Width:1500mm-4200mm
Length:3000mm-18000mm
Heat Treatment:Quenched and Tempered
Technical Requirements & Additional Services:
High tension test
Z-Test (Z15,Z25,Z35)
Low temperature impacting test
Ultrasonic test under ASTM A435,A577,A578
Cetificated by ABS,LR,GL,BV,DNV,KR,NK,CCS,RINA
Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
Shot blasting and Painting,Cutting and welding as per end user's demands
Chemical Composition
|
DNV E500 extra high Strength Chemical Composition |
|||||||
|
Grade |
The Element Max (%) |
||||||
|
C |
Si |
Mn |
P |
S |
Al |
N |
|
|
DNV E500 |
0.20 |
0.10-0.55 |
1.7 |
0.030 |
0.030 |
0.015-0.08 |
0.020 |
|
Nb |
V |
Ti |
Cu |
B |
Ni |
Mo |
|
|
0.02-0.05 |
0.04-0.10 |
0.02 |
|
0.005 |
|
|
|
Mechanical Property
|
DNV E500 extra high general strength property |
|||||||
|
Grade |
|
Mechanical Property |
Charpy V Impact Test |
||||
|
Thickness |
Yield |
Tensile |
Elongation |
Degree |
Energy 1 |
Energy 2 |
|
|
DNV E500 |
mm |
Min Mpa |
Mpa |
Min % |
-40 |
J |
J |
|
t≤50 |
500 |
610-770 |
16% |
33 |
50 |
||
|
50<t≤70 |
500 |
610-770 |
16% |
33 |
50 |
||
|
70<t≤150 |
500 |
610-770 |
16% |
33 |
50 |
||
|
Note: Energy 1 is transverse impact test, Energy 2 is longitudinal |
|||||||