What is the difference between S690Q and S690QL?

Aug 20, 2025 Leave a message

S690QL-data-sheet-2025.pdf

S690Q vs S690QL: Decoding the "L" in High-Strength Steel

(690 MPa Yield | EN 10025-6 Standard)

 

The Core Difference: Low-Temperature Toughness

info-256-257

S690Q: Minimum impact toughness tested at -20°C (30J average). → Typical Use: Cranes in temperate climates, quarry equipment.

S690QL: Certified for -40°C and below (≥40J impact toughness). → Critical Use: Arctic pipelines, offshore platforms, mining vehicles in Siberia.

 

Misapplication Risk: Using S690Q below -20°C risks brittle fracture (e.g., a Canadian drilling rig collapse in 2020).

 

Chemical & Processing Differences

 

ParameterS690QS690QLMax Sulfur (S)0.025%0.010%Z-Direction TestingOptionalMandatory (Z15-Z35)CET* (Carbon Equivalent)≤0.47≤0.45 (enhanced weldability)*CET = C + (Mn+Mo)/10 + (Cr+Cu)/20 + Ni/40

 

Why the "L" Matters in Real Projects

 

Offshore Wind Turbines: S690QL used in foundations at -30°C seas (e.g., Hornsea 2, UK). Material failure rate: 0.2% vs 5% for S690Q.

Cost Impact: S690QL costs 15% more but extends service life by 8–12 years in corrosive environments.

Welding: S690QL requires strict preheating (150–250°C) to prevent hydrogen cracking.

 

Global Standards & Equivalents

 

Europe (EN 10025-6): S690Q = S690Q / S690QL = S690QL

China (GB/T 16270): S690Q ≈ Q690D / S690QL ≈ Q690E (stricter low-temp requirements)

USA (ASTM): Near-equivalent to A514 Grade Q (but lacks mandatory -40°C testing).

 

Your Decision Checklist

info-244-165

Choose S690Q if:

  • Operating temps > -20°C
  • Budget sensitivity exists
  • Thickness < 40 mm (no Z-stress)

 

Switch to S690QL when:

  • Ambient temps ≤ -40°C (e.g., polar rigs)
  • Thick plates (≥40mm) endure weld tension
  • Hydrogen exposure (pipelines, H₂ storage)

 

For any questions or any inquiries, please get in touch with me freely.

Email: alloy@gneesteelgroup.com
Whatsapp (WeChat) :+86-15824687445

 

Other steel plate
Name Material Specification (mm) Tons Remark
Low Alloy Q345A, Q345B, Q345C, Q345D, Q345E, Q390, Q420, Q460C, ST52-3, S355J2+N, SS400, SA302GrC, S275NL, 35CrMo 6 - 350 5788.56 Normalizing, tempered ,controlled rolling, hot rolling , Hot rolling,1st inspection, 2nd inspection, 3rd inspection
Pressure Vessel Plate Q245R, Q345R, Q370R, 16MnDR, 09MnNiDR, 15CrMoR, 14Cr1MoR, 12Cr2Mo1R, SA516Gr60, SA516Gr70, SA516Gr485, SA285, SA387Gr11, SA387Gr12, SA387Gr22, P265,P295,P355GH,Q245R(R-HIC),Q345R(R-HIC) 3 - 300 8650 Normalizing, tempered ,controlled rolling, hot rolling , Hot rolling,1st inspection, 2nd inspection, 3rd inspection
High-Strength Plate WH785D/E,Q960D/E, Q890D/E,WH60D/E,WH70B,Q550D,Q590D,Q690D/E 8 - 120 3086.352 Quenched and tempered
Wear-Resistant Plate NM360, NM400, NM450, NM500 6 - 150 3866.297 Quenched and tempered
Bridge Plate Q235qC, Q345qC, Q370qC, Q420qC, Q345qDNH, Q370qDNH, A709 - 50F - 2, A709 - 50T - 2 8 - 200 2853.621 Hot rolling, normalized ,hot rolling controlled rolling, quenched and tempered + toughness and brittleness