What Is ASTM A573 Grade 70 Steel Plate?
ASTM A573 Grade 70 is a structural quality carbon-manganese-silicon steel plate produced under ASTM A573/A573M. The specification covers three grades, 58, 65 and 70, which are differentiated by the minimum tensile strength they must reach, and Grade 70 is the highest strength grade of the family. The material is intended primarily for structural applications at atmospheric temperatures where improved toughness is required compared with ordinary structural carbon steel.
Because the chemistry is a straightforward carbon-manganese-silicon design, the plate combines predictable strength with good forming and welding behaviour. That makes it a common choice for welded structures, storage tanks and general industrial fabrication, and it is frequently supplied with surface preparation and a full material certificate so that the fabricator can trace each plate back to the melting heat.
Chemical Composition of ASTM A573 Grade 70
The composition limits for the grade are listed below. Carbon, phosphorus and sulfur are held at low levels to preserve toughness and weldability, while manganese provides the strength and silicon contributes to deoxidation.
| Element | Limit (%) | Notes |
|---|---|---|
| C, max | 0.28 | May be adjusted with plate thickness and heat treatment practice |
| Mn | 0.85-1.20 | Provides strength and hardenability |
| P, max | 0.04 | Restricted for toughness and weldability |
| S, max | 0.05 | Restricted to limit hot cracking and inclusions |
| Si | 0.15-0.40 | Deoxidation and strengthening |
| Fe | Balance | Approximately 98% of the mass |
Mechanical Properties of ASTM A573 Grade 70
Tension testing is performed on specimens taken from the plate and the results are reported on the mill certificate. The requirement for the grade is a minimum yield strength of 290 MPa and an ultimate tensile strength between 485 MPa and 620 MPa, with a minimum elongation of 18% measured over a 200 mm gauge length. Because the grade is a structural quality steel rather than a pressure vessel steel, the property set is specified for design at atmospheric temperature.
| Property | Value | Unit |
|---|---|---|
| Tensile strength, ultimate | 485-620 | MPa |
| Tensile strength, yield, min | 290 | MPa |
| Elongation, min | 18 | % in 200 mm |
| Density | 7.85 | g/cm3 |
| Elastic modulus, typical | 200 | GPa |
Key Characteristics in Service
Weldability: good weldability with conventional arc processes, using consumables matched to the strength of the base plate and standard preheat practice for the thickness involved.
Toughness: improved toughness compared with ordinary structural carbon steel, which supports use in tanks and structures exposed to low ambient temperatures.
Formability: sufficient ductility for cold forming, rolling and bending of shells, stiffeners and structural members.
Consistency: a narrow analysis window keeps strength and toughness uniform from heat to heat, so fabrication procedures qualified on one delivery remain valid for the next.
Surface condition: plate can be supplied as-rolled, shot blasted or shot blasted and primed for corrosion protection during storage.
Typical Applications
A573 Grade 70 plate is used for pressure vessels and storage tanks, industrial structural frameworks, machine bases, transport and lifting equipment, and general fabrication in the oil and gas, chemical and manufacturing industries. It is also used for welded pipe, tank shell courses and structural members where a modest strength increase over plain carbon structural steel is useful and where the material will operate at atmospheric temperature.
Ordering, Documentation and Quality Control
When the material is ordered, the purchase order should state the specification and grade, the plate dimensions, the delivery condition and any supplementary requirements such as ultrasonic examination, impact testing or through-thickness testing. Each delivery is accompanied by a material test certificate issued to EN 10204 type 3.1, which records the heat number, chemical analysis, heat treatment and mechanical test results of the actual plates supplied. Additional inspection by an independent third party can be arranged when a project specification requires witnessed testing, and product analysis can be reported alongside the heat analysis when the fabricator needs to confirm the delivered plate rather than the cast.
FAQ
Q: What does Grade 70 mean in ASTM A573?
The number identifies the strength level of the grade. Grade 70 is the highest of the three grades in the specification and requires a minimum tensile strength of 70 ksi, equivalent to about 485 MPa, with a yield strength of at least 290 MPa.
Q: Is ASTM A573 Grade 70 a pressure vessel steel?
It is a structural quality plate intended primarily for structural duty at atmospheric temperature. Where a pressure vessel design code demands a dedicated pressure vessel specification, a grade such as ASTM A516 is normally selected instead.
Q: What is the carbon content and why does it matter?
Carbon is limited to 0.28% maximum. Keeping carbon at that level holds the carbon equivalent low, which limits hardening in the heat affected zone and allows welding without excessive preheat on moderate thicknesses.
Q: Can the plate be supplied shot blasted?
Yes. Shot blasting and priming can be arranged in the processing plant when the plates will be stored outdoors or when the paint system has to be applied before fabrication.
Q: What certificate is issued with the plates?
A mill test certificate to EN 10204 type 3.1 is issued for each delivery. It carries the heat number, the chemical analysis of the heat and the mechanical results of the plates actually supplied, so the material can be traced easily.
Q: Is impact testing required for this grade?
Impact testing is not part of the basic requirement of the grade. Charpy V-notch testing at an agreed temperature can be added as a supplementary requirement when service conditions or the project specification call for it.