A283 Grade C vs. A36 Steel, A572 Grade 50, A516 Grade 70

Aug 21, 2025 Leave a message

ASTM-A572-A572M.pdf

A283 Grade C vs. A36 Steel

info-252-195

Both A283 Grade C and A36 steel have similar chemical compositions, with carbon content ranging from 0.18% to 0.27%, manganese content ranging from 0.60% to 0.90%, and small amounts of other elements.

The main difference between these two grades is their tensile strength, where A283 Grade C has a minimum tensile strength of 55,000 psi (380 MPa), while A36 steel has a minimum tensile strength of 58,000–80,000 psi (400–550 MPa).

A283 Grade C is typically used for general structural purposes, whereas A36 is used in a wider range of applications, including construction of buildings and bridges.

 

A283 Grade C vs. A572 Grade 50 Steel

 

A572 Grade 50 is a high-strength, low-alloy steel plate used in structural applications such as bridges and buildings.

A572 Grade 50 has a higher tensile strength than A283 Grade C, with a minimum yield strength of 50,000 psi (345 MPa) and a minimum tensile strength of 65,000 psi (450 MPa).

A572 Grade 50 also contains alloying elements such as vanadium and columbium to enhance its properties further.

A283 Grade C is considered a lower-strength carbon steel in comparison, suitable for less demanding applications.

 

A283 Grade C vs. A516 Grade 70 Steel

 

A516 Grade 70 is a pressure vessel-quality, carbon steel plate used for moderate and lower-temperature service in pressure vessels. It has a higher tensile strength and yield strength compared to A283 Grade C, with a minimum tensile strength of 70,000 psi (485 MPa) and a minimum yield strength of 38,000 psi (260 MPa).

A516 Grade 70 is primarily used in applications where elevated temperatures and pressure are involved, such as in the petrochemical and oil and gas industries.

On the other hand, A283 Grade C is used for general structural applications and is not suitable for pressure vessel applications.

 

info-256-173

In summary, A283 Grade C steel is a low- to intermediate-tensile-strength carbon steel plate used primarily for general structural purposes. While it shares some similarities with other grades, like A36, it has distinct differences in terms of tensile strength, yield strength, and specific applications. When selecting a steel grade, it's essential to consider the specific requirements of the intended application to ensure the material's suitability.

 

Email: alloy@gneesteelgroup.com
Whatsapp (WeChat) :+86-15824687445

 

FAQ

Q: What is the difference between A36 and A516 steel?

A: It is known for its excellent notch toughness and resistance to brittle fracture. A36 is a general-purpose carbon steel grade suitable for structural applications, while A516 is specifically designed for pressure vessel applications and offers superior notch toughness.

Q: What is ASTM A516 grade 70 equivalent to?

A: P355GH
ASTM A516 GD 70 - Pressure Vessel Steel
A516 GD70 steel plate is equivalent to the P355GH and 490B grades.

Q: What is ASTM A36 steel equivalent to?

A: The ASTM A36 plate is equivalent to grades like ASTM A283C, JIS G3101 SS400, JIS G3106 SM400A, EN10025-2 S235JR, DIN17100 ST37-2, and FE360B.

Q: What is ASTM A36 steel used for?

A: ASTM A36 is used in bolted, riveted, or welded construction projects such as bridges and buildings, it is also used in forming tanks & bins and machined parts like bearing plates, fixtures, rings, and parts for agricultural equipment.

Q: What is ASTM A283 material?

A: A283 refers to a carbon steel plate that conforms to the specifications set forth by the ASTM A283/A283M standard. This standard covers low and intermediate tensile strength carbon steel plates intended for general intermediate-strength usage.

Q: What is the difference between ASTM A283 Grade C and A36?

A: The main difference between these two grades is their tensile strength, where A283 Grade C has a minimum tensile strength of 55,000 psi (380 MPa), while A36 steel has a minimum tensile strength of 58,000–80,000 psi (400–550 MPa)

Q: What is ASTM A572 material?

A: ASTM A572 steel plate is a popular grade of high-strength low-alloy (HSLA) steel that is typically used in structural applications. A572 steel contains chemical alloys that enhance the material's hardness and ability to bear weight, and this material is lightweight relative to steel grades with similar compositions.

Q: What is the difference between ASTM A572 and s355?

A: For mechanical properties, EN S355JR tensile strength is 470-630Mpa,yield strength above 345Mpa. Min. tensile strength of ASTM A572 Grade 50 is 450Mpa, yield strength is above 345Mpa. Generally speaking, they can meet demands of each other.

 

Other steel plate
Name Material Specification (mm) Tons Remark
Low Alloy Q345A, Q345B, Q345C, Q345D, Q345E, Q390, Q420, Q460C, ST52-3, S355J2+N, SS400, SA302GrC, S275NL, 35CrMo 6 - 350 5788.56 Normalizing, tempered ,controlled rolling, hot rolling , Hot rolling,1st inspection, 2nd inspection, 3rd inspection
Pressure Vessel Plate Q245R, Q345R, Q370R, 16MnDR, 09MnNiDR, 15CrMoR, 14Cr1MoR, 12Cr2Mo1R, SA516Gr60, SA516Gr70, SA516Gr485, SA285, SA387Gr11, SA387Gr12, SA387Gr22, P265,P295,P355GH,Q245R(R-HIC),Q345R(R-HIC) 3 - 300 8650 Normalizing, tempered ,controlled rolling, hot rolling , Hot rolling,1st inspection, 2nd inspection, 3rd inspection
High-Strength Plate WH785D/E,Q960D/E, Q890D/E,WH60D/E,WH70B,Q550D,Q590D,Q690D/E 8 - 120 3086.352 Quenched and tempered
Wear-Resistant Plate NM360, NM400, NM450, NM500 6 - 150 3866.297 Quenched and tempered
Bridge Plate Q235qC, Q345qC, Q370qC, Q420qC, Q345qDNH, Q370qDNH, A709 - 50F - 2, A709 - 50T - 2 8 - 200 2853.621 Hot rolling, normalized ,hot rolling controlled rolling, quenched and tempered + toughness and brittleness