1.7225 42CrMo4 +QT AISI 4137 AISI 4140 — quenched and tempered

Aug 28, 2025 Leave a message

The material 1.7225 | 42CrMo4 is an alloyed engineering steel, which has a high strength and toughness.

 

42CrMo4/DIN 1.7225 Alloy Steel manufacturers and suppliers, supplied with round rods,square/flat bars,rollers,shafts,blocks and forging pieces.

42CrMo4/DIN 1.7225 steel is a commonly used grade contains Chromium-Molybdenum elements in European standard EN10083 and EN10250. This steel has good strength and toughness,and good low-temperature impact toughness which are mostly used after quenched and tempered heat treatment. DIN 1.7225 / 42CrMo4 is widely used in large size and important parts,such as axle,gear,connecting rod,engine cylinder,spring,oil drill pipe joints and pinions.

42CrMo4 Forged round bar

1.1.7225 42CrMo4 +QT AISI 4137 AISI 4140  Chemical Analysis 

Grade C Si Mn P S Cr Mo
42CrMo4/1.7225 0.38-0.45 ≤ 0.4 0.6-0.9 ≤ 0.025 ≤ 0.035 0.9-1.2 0.15-0.3
4140 0.38-0.43 0.15-0.35 0.75-1.0 ≤0.035 ≤0.035 0.8-1.1 0.15-0.25

 

2.Related Specifications

AISI:4140/4137 

ASTM:ASTM A331
JIS:SCM440
BS:EN19/708M40
GB:42CrMo

AFNOR:42CD4

 

42CrMo4 Steel Normalizinging Details
1.Normalize temperature:850-880℃
2.Three steps for temperature raising.
3.Proper holding time depends on the dimension.
4.Air cooling.

 

42CrMo4-Mechanical Property With Normalizing

Tensile Strength Yield Strength Elongation Reduction of Area Impact Charpy-V Hardness
≥1020Mpa ≥655Mpa ≥17.7% ≥47% ≥23J 302HBW

42CrMo4 Annealing Diagram

42CrMo4 Annealing Diagram

 

42CrMo4 Steel Annealing Details
1.Annealing temperature:680-720℃
2.Enough time for temperature holding
3.Cooling in the furnace.
4.Max hardness:229HB

42CrMo4-Mechanical Property With Annealing

Tensile Strength Yield Strength Elongation Reduction of Area Impact Charpy-V Hardness
≥655Mpa ≥415Mpa ≥25.7% ≥57% ≥55J 197HBW

42CrMo4 Quenching diagram

42CrMo4 Quenching Diagram

 

Quenching Details
1.Quench temperature:820-880℃
2.Three steps of temperature raising for evenly heating.
3.Hold suitable time for the steel to be thoroughly heated.
4.Oil or Water Quench.
5.Tempering immediately after quenched.

42CrMo4 Tempering diagram

42CrMo4 Tempering Diagram

Tempering Details
1.Temper temperature:540-680℃
2.Air cooling.

 

42CrMo4-Mechanical Property With Quenching and Tempering

Size mm Tensile,Mpa Yield,Mpa Elongation,% Reduction,% Charpy Impact,J Hardness,HB Sample location
Φ230 804 604 23.5 57 +20℃,90 270 1/3 Radius
Φ310 879 677 19.5 57 +20℃,62 290 1/3 Radius
Φ450 803 566 20.5 48 +20℃,54 258 1/3 Radius
Φ540 718 533 21 54 +20℃,56 260 1/3 Radius
Φ700 760 548 19 55 -20℃,28 255 1/3 Radius

 

Supply Size & Condition

Form of Supply Size(mm)
Round bar Φ16-Φ1,000
Square bar Thinkness:Max 800
Flat bar/Blcoks Thickness :120-800
Width:120-1,500

Heat treatment:Normalized / Annealed / Q&T
Surface finish:Black / Rough turned / Peeled